Frit-Happens !

Lampwork => COE 104 => Topic started by: beadammed on May 25, 2010, 09:09:22 PM

Title: Purple???
Post by: beadammed on May 25, 2010, 09:09:22 PM
Can anyone recommend any deep purple opaque glass????????
Title: Re: Purple???
Post by: suzielaws on May 25, 2010, 09:15:35 PM
I love CIM Lapis it is very lovely.
Title: Re: Purple???
Post by: princess pink on May 25, 2010, 09:20:45 PM
i also love grape ape (cim)
Title: Re: Purple???
Post by: Kaz on May 25, 2010, 09:21:36 PM
All the CIMs - evil queen, thai orchid as well as those mentioned above.
Kazx
Title: Re: Purple???
Post by: theflyingbedstead on May 25, 2010, 09:46:22 PM
I adore CiM Eggplant, Blackcurrent and Effetre Dark Silver Plum.
Title: Re: Purple???
Post by: AnnaSpanna on May 25, 2010, 10:18:33 PM
I love blackcurrant - but I haven't successfully managed to encase it and it also does go more purple once annealed - it looks quite black before annealing. It is generally very dark though.
Title: Re: Purple???
Post by: Jolene on May 25, 2010, 10:31:39 PM
I lurve all the CiM purples...not a bad un in the bunch
Title: Re: Purple???
Post by: sea-thistle on May 26, 2010, 01:20:46 AM
I love CIM Poi, Eggplant,Grape Ape! The Effetre handmade violet and purple glass is lovely too! :)
Title: Re: Purple???
Post by: beadammed on May 26, 2010, 08:02:48 PM
Thanks everyone.  I've got a purple and white outfit for my daughter's graduation so I want a deep purple to match.
Title: Re: Purple???
Post by: greenbeadenvy on May 26, 2010, 08:40:00 PM
If you take a photo of it for me hun, I will colour match it for you. Just pm it to me and my beady eye will do the rest ;)
Title: Re: Purple???
Post by: beadammed on May 26, 2010, 09:20:20 PM
Thanks for the kind offer Emma but too late I'm afraid!!!!!!!!!!!!! I went off & bought grape ape & blackcurrant.  As well as other VERY necessary bits and bobs from Martin I'm afraid.  I'll keep it in mind if they don't match tho.
Title: Re: Purple???
Post by: greenbeadenvy on May 26, 2010, 09:26:27 PM
Quote from: beadammed on May 26, 2010, 09:20:20 PM
Thanks for the kind offer Emma but too late I'm afraid!!!!!!!!!!!!! I went off & bought grape ape & blackcurrant.  As well as other VERY necessary bits and bobs from Martin I'm afraid.  I'll keep it in mind if they don't match tho.
When did you buy them? did I pack it? LOL
Title: Re: Purple???
Post by: beadammed on May 26, 2010, 09:35:34 PM
5 minutes ago  ;D ;D ;D I'll try to get my daughter to take a photo tonight to see what u think.
Title: Re: Purple???
Post by: greenbeadenvy on May 26, 2010, 10:40:45 PM
Right you are  :)