Frit-Happens !

Lampwork => COE 104 => Topic started by: puffin on May 10, 2010, 10:06:01 AM

Title: can you use Reichenbach with Effetre
Post by: puffin on May 10, 2010, 10:06:01 AM
stupid question I know but I am just checking . Can you use Reichenbach with Effetre say if I wanted to try and encase a Reichenbach could I use 006 clear. ?

I am making a mess of it all at the moment what with rubbish gravity , over striking so it looks pants. So I might as well have a go at the encasing while I am on a roll  :P

But no really I was afraid to mix that glass just incase it exploded even though it is a 104 glass.
I know not to mix bullseye 90 so just want to be sure.

Title: Re: can you use Reichenbach with Effetre
Post by: Lush! on May 10, 2010, 10:09:05 AM
Yes Stacey, you can mix Reichenbach 104 with Effetre.  ;D
Title: Re: can you use Reichenbach with Effetre
Post by: puffin on May 10, 2010, 10:18:56 AM
thank you