Frit-Happens !

Lampwork => Lampworking Tip n Tricks => Topic started by: helbels on May 09, 2010, 09:14:22 PM

Title: White spots on beads went funny colours after etching...?
Post by: helbels on May 09, 2010, 09:14:22 PM
Hi there

I made some basic pink beads (transparent) on Saturday with some white dots on them - pretty standard stuff.  When I etched them, the bead release has made the edges of the white dots go a sort of rusty brown colour in some places, and no matter how hard I scrub the colour won't come off.

My bead release is at the stage where it's starting to look like Cola.  Do you think this is why?  Should I be replacing it?

Thanks
Helen x
Title: Re: White spots on beads went funny colours after etching...?
Post by: Dragonfire Glass on May 09, 2010, 10:01:51 PM
Mine looks like cola but I haven't noticed it discolour any beads  ???
Title: Re: White spots on beads went funny colours after etching...?
Post by: sarah t on May 10, 2010, 08:48:21 AM
i always clean my beads before etching .......or did you mean the etch fluid is like cola ?
Title: Re: White spots on beads went funny colours after etching...?
Post by: Lush! on May 10, 2010, 10:10:36 AM
I'm assuming you mean etching fluid, not bead release? 

I don't think my etching fluid has ever affected the colour (in a bad way!) even when it gets a bit old and cola-looking.

Any chance of a pic?
Title: Re: White spots on beads went funny colours after etching...?
Post by: Dragonfire Glass on May 10, 2010, 11:59:51 AM
Sorry - bead release is bead release colour, etching fluid looks like cola  ;D