Frit-Happens !

Lampwork => COE 104 => Topic started by: mad bunny on April 24, 2010, 05:21:20 PM

Title: effetre intense black 066
Post by: mad bunny on April 24, 2010, 05:21:20 PM
I really want to try some of this black, does anyone know where I can get some please  :)
Title: Re: effetre intense black 066
Post by: Dragonfire Glass on April 24, 2010, 05:41:53 PM
erm .... Martin?
Title: Re: effetre intense black 066
Post by: beadammed on April 24, 2010, 05:52:54 PM
I got some recently from Sean at OffMandrel.
Title: Re: effetre intense black 066
Post by: mad bunny on April 24, 2010, 05:57:50 PM
Martin hasn't got any and Sean's sold out  :'(
Title: Re: effetre intense black 066
Post by: Shirley on April 24, 2010, 06:02:51 PM
If you were looking for it because you wanted a good solid black try CIM Hades or Tuxedo instead. If you want a black that will web I've got a feeling Hades might but I'm not sure. Haven't tried it myself.
Title: Re: effetre intense black 066
Post by: mad bunny on April 24, 2010, 06:12:09 PM
Quote from: Shirley on April 24, 2010, 06:02:51 PM
If you were looking for it because you wanted a good solid black try CIM Hades or Tuxedo instead. If you want a black that will web I've got a feeling Hades might but I'm not sure. Haven't tried it myself.

I was wanting to try it for it's special effects.  I do have some Hades I will give that a try next time and let you know  ;)
Title: Re: effetre intense black 066
Post by: ♥♥Tan♥♥ on April 24, 2010, 06:20:00 PM
Doesn't the new Reichenbach black web?
Title: Re: effetre intense black 066
Post by: greenbeadenvy on April 25, 2010, 11:34:16 AM
Quote from: Tan on April 24, 2010, 06:20:00 PM
Doesn't the new Reichenbach black web?
yes the deep black does though I'm not sure it webs quiet as much as the intense black.
Title: Re: effetre intense black 066
Post by: helenfc on April 25, 2010, 11:47:42 AM
if you make silvered hades stringer it webs all luverly :)
Title: Re: effetre intense black 066
Post by: mad bunny on April 25, 2010, 03:23:23 PM
Quote from: helenfc on April 25, 2010, 11:47:42 AM
if you make silvered hades stringer it webs all luverly :)

Mmm that sounds interesting thank you  ;)  You know I really need to play around more and get adventurous with my glass  ::)
Title: Re: effetre intense black 066
Post by: fionaess on April 25, 2010, 05:58:29 PM
Hades webs over dark ivory and coral
Title: Re: effetre intense black 066
Post by: AnnaSpanna on April 25, 2010, 06:38:19 PM
I got mine from off-mandrel but it was a few months ago. It was the only place I could find it at the time.
Title: Re: effetre intense black 066
Post by: julieHB on April 25, 2010, 06:47:47 PM
Q stocks it  :) https://sslrelay.com/s194998497.oneandoneshop.co.uk/sess/utn154bd47fff0886a/shopdata/index.shopscript
Title: Re: effetre intense black 066
Post by: mad bunny on April 26, 2010, 10:54:35 AM
Thank you all, Emma has a rod I can try  ;D  Thank you Emma  :-*