Frit-Happens !

Lampwork => COE 104 => Topic started by: puffin on April 23, 2010, 08:09:56 PM

Title: Fuchsia Pink Glass
Post by: puffin on April 23, 2010, 08:09:56 PM

I am after that fuchsia pink glass I could not find on tuffnells or off mandrel , or am i not looking in the right place .

Not baby pink or pink so it is near to purple but Pink that kind of pink dark and lush.
Title: Re: Fuchsia Pink Glass
Post by: hollergrafik on April 23, 2010, 08:14:14 PM
rubiono oro or CIM cranberry pink, both are transparent, there isnt a opaque bright pink in 104
Title: Re: Fuchsia Pink Glass
Post by: Shirley on April 23, 2010, 08:19:41 PM
Try layering rubino over a blue - periwinkle is good.

Title: Re: Fuchsia Pink Glass
Post by: Magpie on April 23, 2010, 08:45:20 PM
Bullseye light fuschia striker (http://off-mandrel.com/index.php?main_page=product_info&cPath=65_88_92&products_id=527) from off mandrel, currently sold out though.
Title: Re: Fuchsia Pink Glass
Post by: Trudi on April 28, 2010, 02:52:19 PM
Ohh you could be after Rubino  - this is a striker, you heat it, it goes clear then gently re-heat to bring out the colour. Work further out in the flame and with slightly more oxygen.

Or less fussy id Reicenbach's Pink Lady! She's a sexy momma!
Title: Re: Fuchsia Pink Glass
Post by: Trudi on April 28, 2010, 02:53:05 PM
Quote from: Magpie on April 23, 2010, 08:45:20 PM
Bullseye light fuschia striker (http://off-mandrel.com/index.php?main_page=product_info&cPath=65_88_92&products_id=527) from off mandrel, currently sold out though.

Tis pretty - I have some of this - but it's 90. I think Stacey is working with 104 at the moment!
Title: Re: Fuchsia Pink Glass
Post by: squirsygirl on April 28, 2010, 04:16:02 PM
I use some r'bach fuchsia frit.  Yummy:

(http://i563.photobucket.com/albums/ss76/squirsygirl/fuchiaflower2.jpg)

I pull it into stringers, and a little goes a long way.

Kirsty
Title: Re: Fuchsia Pink Glass
Post by: Trudi on April 28, 2010, 05:04:38 PM
what a beauty!
Title: Re: Fuchsia Pink Glass
Post by: BeadyBugs on April 28, 2010, 05:27:49 PM
Lovely bead Kirsty!   :)

Yes, as Helen says, if it's a really bright pink you're after, Bullseye might be the way to go.  They seem to have the brightest pinks, and they behave really well in the flame, even I can get them to stay pink and I usually nuke pinks to a lovely brown shade for fun.  :D  Excuse the dodgy bead, but this was made with one of the Bullseye opals and possibly the trans light pink striker.  I think it was this one (http://www.warm-glass.co.uk/Shop/ProductDetails.aspx?ProductId=2029), but I got it in a mixed Bullseye bundle, so I may be wrong.  Warm Glass (http://www.warm-glass.co.uk/Shop/CategoryProducts.aspx?CategoryId=59) usually have some.

(https://i.ibb.co/d27JqDc/Dreadpink-M.jpg)

HP x
Title: Re: Fuchsia Pink Glass
Post by: BeadyBugs on April 28, 2010, 05:32:11 PM
Oops - just seen Trudi's post.  Sorry, yes it is a COE 90 glass, so can't be mixed with 104, but it can be annealed on the same kiln schedule.

Hope you find some pink!!!!!

HP x
Title: Re: Fuchsia Pink Glass
Post by: Trudi on April 28, 2010, 06:19:22 PM
tis a beauty Helen
Title: Re: Fuchsia Pink Glass
Post by: Magpie on April 28, 2010, 08:33:50 PM
Yes that bead is totally dodgy and truly horrendous, if you send it to me I'm sure I can dispose of it safely so it doesn't harm anyone.  ;)


*Goes off to look up the colour*
Title: Re: Fuchsia Pink Glass
Post by: BeadyBugs on April 28, 2010, 09:17:35 PM
 ;D ;D ;D :D

HP xxx
Title: Re: Fuchsia Pink Glass
Post by: squirsygirl on April 29, 2010, 07:03:02 AM
Quote from: Helen P on April 28, 2010, 05:27:49 PM
Lovely bead Kirsty!   :)

Yes, as Helen says, if it's a really bright pink you're after, Bullseye might be the way to go.  They seem to have the brightest pinks, and they behave really well in the flame, even I can get them to stay pink and I usually nuke pinks to a lovely brown shade for fun.  :D  Excuse the dodgy bead, but this was made with one of the Bullseye opals and possibly the trans light pink striker.  I think it was this one (http://www.warm-glass.co.uk/Shop/ProductDetails.aspx?ProductId=2029), but I got it in a mixed Bullseye bundle, so I may be wrong.  Warm Glass (http://www.warm-glass.co.uk/Shop/CategoryProducts.aspx?CategoryId=59) usually have some.

(http://i154.photobucket.com/albums/s250/BeadyBugs/FH%20images/DreadpinkM.jpg)

HP x

I'm off to buy some Bullseye - that's stunning!

K
Title: Re: Fuchsia Pink Glass
Post by: kaatje on April 29, 2010, 07:20:46 AM
Oh my........ I think I have to get me some BE as well.......... what a lovely pink is that!

Title: Re: Fuchsia Pink Glass
Post by: Pandanimal on April 29, 2010, 07:55:49 AM
Quote from: squirsygirl on April 28, 2010, 04:16:02 PM
I use some r'bach fuchsia frit.  Yummy:

(http://i563.photobucket.com/albums/ss76/squirsygirl/fuchiaflower2.jpg)

I pull it into stringers, and a little goes a long way.

Kirsty

Like this one. lovely pink
Title: Re: Fuchsia Pink Glass
Post by: Karen on April 29, 2010, 10:13:29 AM
 ::) just what I need another glass suppler to look at lol
Title: Re: Fuchsia Pink Glass
Post by: squirsygirl on April 29, 2010, 01:21:28 PM
Quote from: Pandanimal on April 29, 2010, 07:55:49 AM
Quote from: squirsygirl on April 28, 2010, 04:16:02 PM
I use some r'bach fuchsia frit.  Yummy:

(http://i563.photobucket.com/albums/ss76/squirsygirl/fuchiaflower2.jpg)

I pull it into stringers, and a little goes a long way.

Kirsty

Like this one. lovely pink

Thanks!  It's r'bach fuchsia over effetre pale pink.

K
Title: Re: Fuchsia Pink Glass
Post by: noora on April 29, 2010, 02:24:01 PM
The bullseye pink striker and violet striker are reason enough to keep a selection of COE 90 rods around the house :)
Title: Re: Fuchsia Pink Glass
Post by: kaatje on April 29, 2010, 06:57:25 PM
For one of my customers I had to make a focal matching a dress of hers.

Maria Louisa advised me to use CIM cranberry pink over white :

(http://i129.photobucket.com/albums/p220/zwadido/fuchsia034.jpg)
Title: Re: Fuchsia Pink Glass
Post by: Trudi on April 29, 2010, 07:43:37 PM
ohhh soo pretty
Title: Re: Fuchsia Pink Glass
Post by: Mand on April 29, 2010, 08:32:36 PM
Beautiful! ;D