Frit-Happens !

Lampwork => Lampworking Tip n Tricks => Topic started by: jammie on April 09, 2010, 03:22:55 PM

Title: gold and silver leaf questions
Post by: jammie on April 09, 2010, 03:22:55 PM
For adding gold leaf to beads, is it better to encase it afterwards. Is it meant to be very slightly raised or rough on the surface once its applied or smooth before leaving as it is or encasing.
What about encasing silver leaf, does it matter whether you do or dont?
Thanks  :)
Title: Re: gold and silver leaf questions
Post by: Lush! on April 09, 2010, 03:34:24 PM
I tend to leave gold leaf on the surface, just very carefully melt it on and kind of blur the edges.

Silver foil is thicker than leaf and easier to leave on the surface, but it will feel a little rough.