Has anyone ever etched any of the mystic colours - and, if so, how did they turn out?
Has anyone etched multicolour - what happens?
Has anyone etched frit beads on a silver foil base - what happens?
Just before I do......
Kazx
Lol! So many questions!! I can only help with multicolour cuz I know Kate (of the sublime nature) etched some mc discs. Will have to find the thread though!
Mystics etch fab - I etch the blue, green and grey regularly ;)
MC looks fab eteched, did a set of 5 button beads.
Thanks folks - I have some lovely mystic beads that have de-vited slightly in a couple of places so I think etching may work out well.
Got to try the MCD too!
Kazx
kaz if the mystic gets the devit around the mandrel give it a nice bathe in mid to top flame until it has a good glow, the devit goes.
Thanks Kay - I'll try that next time!
In the meantime, they etched nicely
(http://farm3.static.flickr.com/2754/4480814159_3a7d933dfd_m.jpg) (http://farm5.static.flickr.com/4024/4480813033_3370dcb7ed_m.jpg)
Kazx
Oh yes, indeed they did! I think the Mystics should be called Velvets instead actually ;D
Gorgeousness Kaz, aren't you glad you asked though ;)
I etched some mc and didnt like it. Will try and post some pics in the next few days.
I just etched some mcd and it looks great! :D
Ooops. I forgot. The ones I etched I sold. So they must not be that bad!! :)