Lampwork => Lampworking Tip n Tricks => Topic started by: emvee on March 29, 2010, 03:56:38 PM

Title: Silver foil
Post by: emvee on March 29, 2010, 03:56:38 PM
I have some EBERHARD FABER silver leaf .Can I use this to make silvered ivory or does it have to be sterling silver leaf?
Title: Re: Silver foil
Post by: chocolateteapot on March 29, 2010, 04:45:48 PM
No idea but u have nothing to lose by having a go ( i hope) .....u will tell when u use it if it is any cop...BUT make sure you have good ventilation whether it works or not ;)Silver has rotten fumes that we shouldnt be inhaling. Wait and see what other replies you get in case its an absolute no no!!!!
Tracy x
Title: Re: Silver foil
Post by: ♥♥Tan♥♥ on March 29, 2010, 04:46:54 PM
I think it might be silver coloured leaf rather than the real thing, have you got enough ivory just to give it a go?
Title: Re: Silver foil
Post by: Kalorlo on March 29, 2010, 04:47:46 PM
It has to be fine silver (999) not sterling silver (925). I think the Eberhard Faber stuff is just silver-coloured. Tuffnell's has the right stuff  ;)

(Edit: Whoops, wrote 995 instead of 925. Nines on the brain!)
Title: Re: Silver foil
Post by: Charli on March 30, 2010, 11:00:10 AM
The fabhard stuff isn't real silver- it just turns to black ash (guess how I know!). The same can be said for most 'metal leaf' sold alongside polymer clay- I've even had the stores swear to me it was all real metal leaf (this was copper), when actually it was really flammable plastic stuff!
Title: Re: Silver foil
Post by: emvee on March 30, 2010, 09:57:38 PM
Thanks to all who replied.At least now I know.Is Tuffnels the only place I can get the real thing?
Title: Re: Silver foil
Post by: Kalorlo on March 30, 2010, 10:05:07 PM
Not the only place - I think most of the lampworking suppliers should have some, and I'm sure there are other places too. Just make sure it says fine silver  ;D