Lampwork => COE 104 => Topic started by: Hazer on March 29, 2010, 02:54:12 PM

Title: Choosing Glass
Post by: Hazer on March 29, 2010, 02:54:12 PM
Not that I'm ready for more glass yet, but for when I am: what colours would you recommend I get for working on a hothead? I'm thinking in the vein of which special glasses that would work, which colour combos are good for newbies, that sort of thing :D
Title: Re: Choosing Glass
Post by: Billie on March 29, 2010, 04:33:23 PM
I would suppose you might want to avoid the stiffer colours on a HH, as they'll take longer to melt - like transparent blue for example.  And thick rods, like some of the lauscha colours... TBH it never bothered me though  :D
Title: Re: Choosing Glass
Post by: chocolateteapot on March 29, 2010, 04:41:40 PM
Triton and Psyche are a treat on a hot head..xxx
Title: Re: Choosing Glass
Post by: ♥♥Tan♥♥ on March 29, 2010, 04:48:20 PM
Yep, avoid anything thick, you will be there forever, trans blues and reds are pretty stiff to work but all the opaque colours are good
Title: Re: Choosing Glass
Post by: Kalorlo on March 29, 2010, 04:53:39 PM
I haven't noticed much problem with transparent blues... Sure, some colours are softer than others, but I wouldn't have thought the difference was enough to avoid them (especially if you like blue!) ;D
Title: Re: Choosing Glass
Post by: ScarletLeonard on March 29, 2010, 06:15:18 PM
I have noticed some are slower than others on the HH but haven't ran into any major problems yet. I'm working my way through the long way round trying a bit of everything thanks to my determination to see it all for myself. So when I do progress to a Minor I know roughly what I can expect from the glass.

I'm sticking to getting my hands on effetre rod selections for the time being, very tempted to try the Reichenbach which I nearly put in with my order today but decided to wait a little longer. (wails that they were so much prettier than the effetre cool colours selection.)

I'm not bothered if I end up with a few 'organic' (I use that term very loosely) if it means in the long run I understand the glass better.

I have probably succeeded in confusing you even more.
Scarlet xx





Title: Re: Choosing Glass
Post by: helbels on March 29, 2010, 06:16:59 PM
With regard to silver glass, you won't go wrong with Psyche, Aurae and Triton as they are reducers, and the Hothead does reducing very nicely :)
Title: Re: Choosing Glass
Post by: Hazer on March 30, 2010, 05:22:50 PM
Okay, so Triton and maybe Pschye and Aurae are definites :D I didn't realise the transparent blues were a bit stiffer - it explains why I had a bit of trouble with them, but I'm stubborn, so I've kept going with them ;) For me it's the yellows that are difficult for some reason.

At the moment, I'm going through the mixed Effetre glass I got with Tufnell's starter pack, but I've realised I'm kinda bad with colour matching, so I have some odd combos...like bright yellow with orangey-red raised dots :(
Title: Re: Choosing Glass
Post by: ♥♥Tan♥♥ on March 30, 2010, 05:44:27 PM
Why are you finding the yellows difficult flower?
Title: Re: Choosing Glass
Post by: Hazer on March 30, 2010, 06:12:03 PM
They just don't seem to melt at all - I spent about ten minutes trying to get one rod properly glowing and moving :( And seeing as my hothead tends to go out every ten to twenty minutes, that meant I got it glowing, then the flame went out before I could make a bead (I torch outside)