Fusing and Stained Glass Tips and FAQ's => Fusing Tips and FAQ's => Bullseye Glass => Topic started by: noora on March 23, 2010, 01:39:45 PM

Title: Bullseye pink, plum and salmon pink "opal" colours
Post by: noora on March 23, 2010, 01:39:45 PM
A while ago I bought some striking "opal" bullseye sheets from Warm Glass: pink, salmon pink and plum. I've tried them in a few different temperatures and ramps, but the colours end up uneven and a bit dull. Are they supposed to be like that or do I need to find better temps/ramps? Any tips?
Title: Re: Bullseye pink, plum and salmon pink "opal" colours
Post by: Zeldazog on March 23, 2010, 08:12:33 PM
I don't recall having trouble with the other two, but I've often had the scummy effect with salmon pink, which I assumed was de-vitrification.  Not had unevenness even with that though?