Frit-Happens !

Lampwork => COE 104 => Topic started by: Kalorlo on March 22, 2010, 10:06:06 AM

Title: Identifying anise white?
Post by: Kalorlo on March 22, 2010, 10:06:06 AM
I have an unlabelled white rod that came in my starter pack that looks very slightly more translucent than my normal white. I tried making a spacer from it - the rod didn't shock, but I was being careful with it, so I don't know if that helps! It felt different to work and my spacer again seems to be very very slightly more translucent, particularly around the holes.

I looked at the fritipedia and it says anise white webs with intense black and goes rusty when super heated. I'll have a go at the latter. I don't have any intense black, but I do have a rod of CiM Hades. Anyone know if that gives the same effect, or if there's anything else I can try?

I'm not sure if I'm just seeing things!
Title: Re: Identifying anise white?
Post by: SilverGems89 on March 22, 2010, 10:36:50 AM
If you have a rod of normal white to compare it to the difference is fairly obvious, it looks slighty more milky/opal, and it is really runny when it gets hot...HTH
Title: Re: Identifying anise white?
Post by: Kalorlo on March 22, 2010, 10:47:02 AM
That's the problem - I *think* it looks different next to the normal rod, but I want a way of making a positive identification!  ;D
Title: Re: Identifying anise white?
Post by: Flyingcheesetoastie on March 22, 2010, 10:57:31 AM
Ask it?  ;D  Ok not helpful, sorry....
Title: Re: Identifying anise white?
Post by: Diane on March 22, 2010, 10:58:42 AM
It spits like mad if it's anise white - very shocky glass - and it does have a different look against the dense white.
Title: Re: Identifying anise white?
Post by: SilverGems89 on March 22, 2010, 11:04:29 AM
Quote from: Flyingcheesetoastie on March 22, 2010, 10:57:31 AM
Ask it?  ;D  Ok not helpful, sorry....
LOL Rachel, i talk to my glass all the time, im only gonna start worrying if it answers back!
Title: Re: Identifying anise white?
Post by: Flyingcheesetoastie on March 22, 2010, 11:08:35 AM
(Gemma, don't put me in the hot thing, PLEEEEASE!!!!)
Title: Re: Identifying anise white?
Post by: Black Heart Beads on March 22, 2010, 11:11:26 AM
My Anise has a small almost clear core and is not much of a talker, but it spits like mad.
Title: Re: Identifying anise white?
Post by: SilverGems89 on March 22, 2010, 12:35:15 PM
Quote from: Flyingcheesetoastie on March 22, 2010, 11:08:35 AM
(Gemma, don't put me in the hot thing, PLEEEEASE!!!!)

OMG my ribs hurt, that made me giggle so much! you know im gonna hear that everytime i go to put a rod in the flame now right?
Title: Re: Identifying anise white?
Post by: Flyingcheesetoastie on March 22, 2010, 12:51:04 PM
(Yeah baby, go on get me red hot and melting....) Naughty Masachistic Rod
Title: Re: Identifying anise white?
Post by: SilverGems89 on March 22, 2010, 01:06:03 PM
ok, now im scared of my glass  :P
Title: Re: Identifying anise white?
Post by: Redhotsal on March 22, 2010, 01:41:52 PM
Yes, it's very shocky, also it's usually much thicker than a "standard" white rod. Pull a little stringer and squiggle some on a normal black bead and let it melt in. If the stringer just sits on the surface and remains opaque it's white but if it sinks in and you get a thin purplish line in the centre of the stringer, in other words a chemical reaction. then you've got anice white.
Title: Re: Identifying anise white?
Post by: Kalorlo on March 22, 2010, 02:01:04 PM
Thanks Sal!
Title: Re: Identifying anise white?
Post by: Yellow friend on March 22, 2010, 04:01:59 PM
Hold it up to the light - if its very slightly transclucent - its anice - its shocky but worth experimenting with, you can get some nice effects if you use it as a base and superheat it - not just with intense black - it works lovely with coral red and aurea.
Title: Re: Identifying anise white?
Post by: silverlemon on March 22, 2010, 05:29:18 PM
This stuff looks so different when hot.

It also feels different in the rod.
Try gently sliding your fingers up and down the rod (ooer missus)  when cold and it feels textured, whereas normal white is silky smooth  ;D
Title: Re: Identifying anise white?
Post by: Yellow friend on March 22, 2010, 05:41:18 PM
Forgot that Sarah - it's another way I tell the difference in the dark too. Its def. not as smooth as 'normal glass'.

Another little tip - for recognising silvered glass - I melt the tip of one end so it shows the silvering and then use it from the other end - this is born of expensive use of Triton as cobalt blue and Aurea as a pink!
Title: Re: Identifying anise white?
Post by: Kalorlo on March 22, 2010, 10:28:12 PM
Ok, I tested tonight with it and white. They're still cooling, but I feel pretty certain saying that it *is* anice, because it definitely sunk in and the normal white didn't. It's also slightly translucent when held up to the light and is a little softer than the normal white.

But! It's still not shocky. It's really nice to melt, actually. And the rod is the same thickness as my white and feels silkier than it does, not rough at all.  ???

Have I miraculously ended up with one rod of the best anice ever? Because if there's any more like this, I really like this glass.
Title: Re: Identifying anise white?
Post by: Carol on March 22, 2010, 10:48:23 PM
You must have some from the same batch as me Heather - I haven't had shocky bother with mine either  ;D
Title: Re: Identifying anise white?
Post by: julieHB on March 22, 2010, 10:51:01 PM
Could be Effetre Opalino white? - looks a bit translucent, almost milky, but is not shocky. Smooth to touch. Lovely glass!
Title: Re: Identifying anise white?
Post by: Kalorlo on March 22, 2010, 11:00:01 PM
I don't know, Julie - it came with my Effetre starter pack from Tuffnell's and I thought they didn't carry the opalinos and alabastros?
Title: Re: Identifying anise white?
Post by: Lush! on March 23, 2010, 12:50:04 AM
I got a batch of anice white very recently, and it's great - not shocky at all.
Title: Re: Identifying anise white?
Post by: Kalorlo on March 23, 2010, 07:39:30 AM
Carol and Lush!Julie - good to know!

Hmm, I already have Flame Off glass orders placed, do I need to add to them...?  ;D
Title: Re: Identifying anise white?
Post by: helenfc on March 23, 2010, 07:41:11 AM
same here heather i have a rod of 208 from the stater pack and its gorgeous to use :)