Frit-Happens !

Lampwork => Lampworking Tip n Tricks => Topic started by: princess pink on February 24, 2010, 10:33:12 PM

Title: best bead release?
Post by: princess pink on February 24, 2010, 10:33:12 PM
Hey

what do you reckon is the best bead release? I'm due for some more and have been using fusion but find it cracks a fair bit.

any other reccommendations? i've tried dirty looie and it was shockingly bad!
Title: Re: best bead release?
Post by: amareargentum on February 24, 2010, 10:37:21 PM
I like Foster Fire - it has worked well whether air or flame dried
Title: Re: best bead release?
Post by: Carol on February 24, 2010, 10:51:13 PM
Quote from: princess pink on February 24, 2010, 10:33:12 PM

any other reccommendations? i've tried dirty looie and it was shockingly bad!

I'm one of the few who seems to like Dirty Looie - sorry I've no other recommendations Shahlaa, but if you stillhave some Dirty Looie left I'd love to do a trade with you :)
Title: Re: best bead release?
Post by: princess pink on February 24, 2010, 10:53:14 PM
Quote from: Carol (fed up with strawackie) on February 24, 2010, 10:51:13 PM
Quote from: princess pink on February 24, 2010, 10:33:12 PM

any other reccommendations? i've tried dirty looie and it was shockingly bad!

I'm one of the few who seems to like Dirty Looie - sorry I've no other recommendations Shahlaa, but if you stillhave some Dirty Looie left I'd love to do a trade with you :)

pm'ed you hun!
Title: Re: best bead release?
Post by: princess pink on February 24, 2010, 10:53:44 PM
where sells foster fire? x
Title: Re: best bead release?
Post by: hollergrafik on February 24, 2010, 10:57:40 PM
Quote from: princess pink on February 24, 2010, 10:53:44 PM
where sells foster fire? x
I got mine from The bead shed http://cgi.ebay.co.uk/FOSTERFIRE-Lampworking-Bead-Release-Small-4oz-REGULAR_W0QQitemZ120436062088QQcmdZViewItemQQptZUK_Crafts_Glass_Art_Supplies_CV?hash=item1c0a8c7788
Title: Re: best bead release?
Post by: princess pink on February 24, 2010, 11:03:47 PM
oo cheers kay, is the heavy duty one for something else?

I'm still not decided so other opinions greatly welcomed!
Title: Re: best bead release?
Post by: amareargentum on February 24, 2010, 11:06:17 PM
I got mine from Q, but the ebay supplier Kay suggests may be quicker and cheaper on postage.
Title: Re: best bead release?
Post by: MangoBeads on February 25, 2010, 08:39:27 AM
Having used all sorts of foster fire I now use Fusion plus for all my big beads and its good n strong - I have it on my webbie .
Title: Re: best bead release?
Post by: fionaess on February 25, 2010, 10:44:34 AM
Foster regular for soft and Best for boro...
Title: Re: best bead release?
Post by: Helen G on February 25, 2010, 10:47:46 AM
I use fusion and since I stopped letting it get really hot (as in glowing mandrel) I don't have many problems. I even make my large focal hearts with it and so far, even though they take nearly 45 mins I haven't had an issue. Sometimes if I've used a press on the same bead more than a couple of times it will crumble off but other than that fine.
Now this is probably tempting fate but I have yet to have a bead that I can't remove from the mandrel either.
Title: Re: best bead release?
Post by: Jennie Lamb on February 25, 2010, 10:58:00 AM
Quote from: MangoBeads on February 25, 2010, 08:39:27 AM
Having used all sorts of foster fire I now use Fusion plus for all my big beads and its good n strong - I have it on my webbie .


I got some from Manda and it is the best I've used in my short time on the torch.  I used to get alot of cracking at the crucial moment and this one holds solid which is SO satisfying!!  Get it from Manda I say!!
Title: Re: best bead release?
Post by: squirsygirl on February 25, 2010, 04:27:45 PM
I use fusion, but have bought some 'bucket of mud' from Frantz.

BoM cleans a lot easier, but have yet to get it to flame dry, I have to dip and air dry in the house where it's warmer.

It's very thick, too.  I have to draw the mandrel out painfully slowly.

Kirsty
Title: Re: best bead release?
Post by: ♥♥Tan♥♥ on February 25, 2010, 04:40:00 PM
I'm a Foster fire girl, I love it and it can take all sorts
Title: Re: best bead release?
Post by: firedinglass on February 26, 2010, 11:11:59 AM
Foster fire, it does seem to dry out in the jar..but a bit of water and i'm OK again!
Title: Re: best bead release?
Post by: Kaz on February 26, 2010, 11:27:15 AM
Quote from: Helen G on February 25, 2010, 10:47:46 AM
I use fusion and since I stopped letting it get really hot (as in glowing mandrel) I don't have many problems. I even make my large focal hearts with it and so far, even though they take nearly 45 mins I haven't had an issue. Sometimes if I've used a press on the same bead more than a couple of times it will crumble off but other than that fine.
Now this is probably tempting fate but I have yet to have a bead that I can't remove from the mandrel either.
Wot she said - never used anything else and love it!
Title: Re: best bead release?
Post by: Redkite on February 26, 2010, 08:32:34 PM
Ditto!