Frit-Happens !

Lampwork => COE 104 => Topic started by: beads-on-toast on April 08, 2007, 04:03:56 PM

Title: encasing frit
Post by: beads-on-toast on April 08, 2007, 04:03:56 PM
what COE rod should i use to encase frit with a COE of about 96?
Thanks
x
Title: Re: encasing frit
Post by: LesleyMac on April 08, 2007, 04:38:18 PM
I would say it depends what the base glass is, if its 104 then you could probably get away with 104 clear, as long as there is not too much frit at 96.
Title: Re: encasing frit
Post by: beads-on-toast on April 08, 2007, 05:15:41 PM
Thats what i thought.
You know when you think, oooh i've read that somewhere.
Could i find where i had read it? NOPE

thanks les