Frit-Happens !

Lampwork => Lampworking Tip n Tricks => Topic started by: Binny on January 30, 2010, 07:42:11 PM

Title: using fine silver wire
Post by: Binny on January 30, 2010, 07:42:11 PM
Hi everyone

Hoping for a little advice, i would like to get myself some silver wire to add some detail to my beads. Just to add some fine lines and little specs on them. i have been on Palmer metals and i am thinking of ordering the fine silver wire on a reel, but it ranges in size from 0.3mm to 2mm as it is very expensive i wanted to be sure to order the right size. They also have gold wire is this to add detail to your beads too.

Thanks Binny :)
Title: Re: using fine silver wire
Post by: turnedlight on January 30, 2010, 08:07:31 PM
The finer the wire the smaller the dots will be on the bead - I have the 0.3mm, it's a good size as it's not too tricky to apply but gives fairly small lines and dots of silver.
Title: Re: using fine silver wire
Post by: Binny on January 30, 2010, 08:11:01 PM
Wow! that was such a quick reply thank you for your advice :)
Title: Re: using fine silver wire
Post by: BeeBeads on January 30, 2010, 08:46:05 PM
I also use the 0.3mm.  It's very manageable and gives good results too.




Bee
Title: Re: using fine silver wire
Post by: Lyn G on January 30, 2010, 11:32:07 PM
Hi Binny,

I get mine from Lynne at The Dragonfly Company.....   www.thedragonflycompany.com/wire.html   

In fact, I have just ordered some more this evening....and I can highly recommend it!   ;D ;D


Lyn


Title: Re: using fine silver wire
Post by: DragonflyLynne on January 31, 2010, 04:12:02 PM
Quote from: Lyn G on January 30, 2010, 11:32:07 PM
Hi Binny,

I get mine from Lynne at The Dragonfly Company.....   www.thedragonflycompany.com/wire.html   

In fact, I have just ordered some more this evening....and I can highly recommend it!   ;D ;D


Lyn


Thanks Lyn! Your wire will be in the post first thing tomorrow (Monday)  ;D
Title: Re: using fine silver wire
Post by: turnedlight on January 31, 2010, 04:58:35 PM
Having said all that, I would like to try an even finer one, to hopefully get even smaller dots etc.
Also, take care with wire wrapped on the outside, I rarely do it now without encasing it, as unfortunately the blobs can come off with wear, especially if they have a slightly spikey end to them, so if I do use it on the outside I tend to marver it down into the glass and check for spikey ends to the blobs. I do love the way it looks though, and maybe it's not so bad with finer wire..
Title: Re: using fine silver wire
Post by: Lyn G on January 31, 2010, 08:29:30 PM
Quote from: DragonflyLynne on January 31, 2010, 04:12:02 PM
Quote from: Lyn G on January 30, 2010, 11:32:07 PM
Hi Binny,

I get mine from Lynne at The Dragonfly Company.....   www.thedragonflycompany.com/wire.html   

In fact, I have just ordered some more this evening....and I can highly recommend it!   ;D ;D


Lyn


Thanks Lyn! Your wire will be in the post first thing tomorrow (Monday)  ;D


Thank you, Lynne.......brilliant service!!   :) :)

Title: Re: using fine silver wire
Post by: Elisa Loves on February 03, 2010, 03:34:59 PM
Thanks Binny, I was just thinking I'd like to give the silver wire a go myself and my question has been answered too!  ;D
Title: Re: using fine silver wire
Post by: Mand on February 04, 2010, 05:21:20 PM
Quote from: Lyn G on January 30, 2010, 11:32:07 PM
Hi Binny,

I get mine from Lynne at The Dragonfly Company.....   www.thedragonflycompany.com/wire.html   

In fact, I have just ordered some more this evening....and I can highly recommend it!   ;D ;D


Lyn




Me too, jolly good service! ;D
Title: Re: using fine silver wire
Post by: DragonflyLynne on February 05, 2010, 04:38:17 PM
Quote from: Mand on February 04, 2010, 05:21:20 PM
Quote from: Lyn G on January 30, 2010, 11:32:07 PM
Hi Binny,

I get mine from Lynne at The Dragonfly Company.....   www.thedragonflycompany.com/wire.html   

In fact, I have just ordered some more this evening....and I can highly recommend it!   ;D ;D


Lyn




Me too, jolly good service! ;D

*blushing*  :)
Title: Re: using fine silver wire
Post by: Binny on February 06, 2010, 10:03:50 AM
Very exited! my silver wire has arrived and i am not working this Sat so i am going to have a go with it  and see how i get on. Even more exiting i have had a parcel delivered from Tuffnells i ordered lots of reactive glass Aion, Psyche, Triton and Kronos and some Silver brown and theirs more! some silver foil! i am going to have so much fun this weekend even though i have spent all my Penny's. I had a lovely mint chocolate too!  Spoke to Emma at Tunnels she was great and gave me some advice on a few things.

Time to go and play!  ;D