Can someone advise me how I paint with frit please?  I've heard this technique mentioned a few times and I can't find any tut's on how to do it.  I suspect it's making a striger out of frit and pinting the stringer on but i'm not sure.  Any help would be most appreciated.

Thanks
Janey x
Title: Re: Painting with frit
Post by: SueP on January 22, 2010, 10:33:22 AM
i've been wondering the same - I often dip a warm rod in frit and melt it in before painting it on the bead so wonder if that's it ???
Title: Re: Painting with frit
Post by: SueP on January 22, 2010, 10:41:18 AM
Thanx for that :)
Title: Re: Painting with frit
Post by: Margram on January 22, 2010, 11:04:58 AM
http://valcoxfrit.com/ (http://valcoxfrit.com/)  Scroll down for the secret ;)
Title: Re: Painting with frit
Post by: lemon kitten on January 22, 2010, 05:01:35 PM
Thanks folks! I've just ordered some of these lovely Val Cox frits!

Janey x
Title: Re: Painting with frit
Post by: Warm Glass UK on January 25, 2010, 12:19:35 PM
We have a one-day Frit & Powder Adventure course and a two-day Painting with Light Foundation course at Warm Glass UK - is this the sort of thing you are interested in?

http://www.warm-glass.co.uk/Shop/CategoryProducts.aspx?CategoryId=108

Pippa

Title: Re: Painting with frit
Post by: Pat from Canvey on January 25, 2010, 10:20:55 PM
Janey, don't forget that Val's frits are COE 96.
Title: Re: Painting with frit
Post by: lemon kitten on January 26, 2010, 08:05:42 AM
Can I use them with standard 104 Effetre and CIM?

Janey x
Title: Re: Painting with frit
Post by: astringofbeads on January 26, 2010, 08:35:16 AM
Yes you can, but they must make up only 5-10% of the glass in the bead, use much more and you could get compatibility problems. Some frits are more forgiving than others ( depends on the lead content I think), and a lot of Val's are rich saturated colours so you should always use less than you think ;)
Title: Re: Painting with frit
Post by: lemon kitten on January 26, 2010, 06:15:26 PM
Thanks for that I'll have a go see what happens

Janey x
Title: Re: Painting with frit
Post by: princess pink on January 26, 2010, 06:41:09 PM
Jaq is it possible to get compatibility problems with the 96 clear you are selling and val's frits? i did the frit painting technique using silver lake and riverdance and a rod of your clear. Out of 6 beads, 2 cracked after cooling, and a further 2 cracked in the kiln. All my other beads are fine. used the frit over some cim and effetre (about 5%) and not probs, just the encased ones. I know i didn't mix up the clears as yours are labelled :) Not sure if i'm doing something wrong but don't often have beads crack on me. :(
Title: Re: Painting with frit
Post by: cwest on January 26, 2010, 06:46:35 PM
Quote from: princess pink on January 26, 2010, 06:41:09 PM
Jaq is it possible to get compatibility problems with the 96 clear you are selling and val's frits? i did the frit painting technique using silver lake and riverdance and a rod of your clear. Out of 6 beads, 2 cracked after cooling, and a further 2 cracked in the kiln. All my other beads are fine. used the frit over some cim and effetre (about 5%) and not probs, just the encased ones. I know i didn't mix up the clears as yours are labelled :) Not sure if i'm doing something wrong but don't often have beads crack on me. :(

I have had this problem too. Thought it was just me.

Carolyn
Title: Re: Painting with frit
Post by: princess pink on January 26, 2010, 07:05:12 PM
Quote from: cwest on January 26, 2010, 06:46:35 PM
Quote from: princess pink on January 26, 2010, 06:41:09 PM
Jaq is it possible to get compatibility problems with the 96 clear you are selling and val's frits? i did the frit painting technique using silver lake and riverdance and a rod of your clear. Out of 6 beads, 2 cracked after cooling, and a further 2 cracked in the kiln. All my other beads are fine. used the frit over some cim and effetre (about 5%) and not probs, just the encased ones. I know i didn't mix up the clears as yours are labelled :) Not sure if i'm doing something wrong but don't often have beads crack on me. :(

I have had this problem too. Thought it was just me.

Carolyn

phew, i'm glad it's not just me!! I never have beads crack, I feel like i've wasted precious glass and frit now :(