Hello all
I have a lentil trio press from Spheres of Glass, which I've owned for a couple of months. At first it seemed fine, but now the darned thing is sticking all the time - sometimes I literally have to use both hands to try to prise the top off the bottom.
Does anyone have any experience of this?
It may be my imagination, but it seems to get worse as the press gets hotter - which is making me wonder if the pins are expanding with the heat. Having said that though, its a bit random - sometimes its fine, and other times awful.
I lost 3 beads tonight because of it. :-[
Any suggestions? I've tried rubbing a bit of olive oil on the locating pins, but it didn't seem to achieve much.
Helen x
In the beginning when I started using presses they sometimes stuck because I put the glass in when it was too hot.
Do you have the chunky lentil press? I think someone else had problems with that sticking, although I have never had any more problems after I learnt that the glass should cool a bit before pressing.
Hope you get it sorted! :)
Hiya
Yes, its the fat lentil press that's sticking. It doesnt seem to matter if I have a lot of glass in the press or just a little bit - the sticking happens randomly and even when completely empty of glass at times >:(
I had the problem with a lentil trio which I had replaced and its mostly fine now. I do have another large lentil press that sticks though, and I agree that it seems worse when hot so I think its got something to do with the pins expanding.
When it happens to me I slide my little veg knife inbetween the plates and twist.
Thanks for that Julie - I have emailed Sandy at Spheres of Glass to see if she has any suggestions, or has had any problems reported. I'm really sad because I love the shape that the fat lentil produces. I hope I can get it sorted, as it's almost unusable at the moment.
I have the same problem with the same press, which kinda stops me from using it.
Good tip though Julie. Some one else suggested to pop in some water to cool it down - bit of a faf though!
I just had an email back from Sandy @ Spheres of Glass saying that she is forwarding my problem on to the engineer who makes them.
She said no one else has reported problems though, that she has a set she uses all the time with no problems, and suggested that it could be me, not removing the top half vertically enough. Surely though, if this was the case, I'd be having the same issue with my other presses (which I'm not).
She suggested putting a bit of WD40 on the pins to see if that helps. Will need to keep it well away from the torch though - isn't WD40 very flammable?? :o
Incidentally Trudi, I did try putting the press in water tonight - seemed to help a bit for about 5 mins, then the problem recurred.
Sounds like the pins are snug in the hole, are they straight or elongated cone shaped? Perhaps they can be filed down a bit..
They start off straight and then taper to a cone. They don't seem to stick all the way along - just at a point about halfway down.
Well I reported it to her - so you're not the first one!
I've just tried a bit of WD40 - seems a bit smoother at the moment but hard to tell until I start making beads again.
Will keep you posted...