Title: simple question really-band round the belly?
Post by: bubblefizz on December 05, 2009, 10:09:48 AM
For ages now ive wondered how you get a thick band/stripe round the belly of a bead
ive tried with a thick and a thin rod, but its always uneven edges  ::)
how do you get it on neatly  ???
Title: Re: simple question really-band round the belly?
Post by: Meagan Lily on December 05, 2009, 10:30:56 AM
I do it by making 3  discs close together and then gently heating them into one, but even then they sometimes get wonky. I don't know how else to do it as my stringer control is non existant.
Title: Re: simple question really-band round the belly?
Post by: helbels on December 05, 2009, 10:37:03 AM
Kay (Hollergrafik) told me a great tip that if you make a barrel out of one colour (eg: white) then put cylinders of another colour on each end (so you bead looks like a dumbell), then heat it, then the dumbell end bits spread and you get a nice thin line of your barrel colour in the middle.  I'm wondering if the fat band you've seen is done in a similar way.....
Title: Re: simple question really-band round the belly?
Post by: bubblefizz on December 05, 2009, 10:40:02 AM
mmm suppose i can give that a try
ive asked the question on LE see what they suggest  ;)
Title: Re: simple question really-band round the belly?
Post by: Helen G on December 05, 2009, 11:58:28 AM
I do it with thick stringer which I usually straighten up using tweezers.
Title: Re: simple question really-band round the belly?
Post by: bubblefizz on December 05, 2009, 02:55:57 PM
thanks helen good tip  ;)