Frit-Happens !

Lampwork => Lampworking Tip n Tricks => Topic started by: Pam on March 26, 2007, 01:43:33 PM

Title: Spot encasing-tell me more
Post by: Pam on March 26, 2007, 01:43:33 PM
I am having a little trouble with florals. I have read some articles on spot encasing, I can guess what it is bit how exactly do you do it.
Also I know I am asking a lot but those that are happy with floral beads can you post a simplified tutorial I am not sure if I need to encase after vine and then again after floral decoration or place floral dots straight on the vine, somehow my flower or vine always seem to bleed though the encasing.
Pam
Title: Re: Spot encasing-tell me more
Post by: MangoBeads on March 26, 2007, 03:11:16 PM
Hi Pam - personally I place dots for petals on top of vine and only encase between flowers or I end up with a huge bead !

Spot encasing is just putting clear over the entire flower not always easy IMO.

Try and keep it simple to start place your vine and your flowers then encase just once - I heata large blob and push it round the cool bead - hope this helps a little bit! Good Luck
Title: Re: Spot encasing-tell me more
Post by: LesleyMac on March 26, 2007, 03:11:43 PM
Don't know about spot encasing but this is how I do flowers.

Make a small bead, roll in frit, add vine whatever.
Encase (thinly if possible)  - important ensure the ends of the encasing are pushed towards the mandrel to avoid any colour seeping through. Melt into shape

Make small dots for flowers, then transparent dots on top of dots for depth (lots of options here, you could even put three dots on top of each other depending on what you are doing)

Melt dots in slowly, shape and let bead cool a bit.

Spot heat centre of flowers and plunge into middle of dots with either tungsten tool or stamen cane or stringer or whatever.

Then I "dump" case, that is melt a big blob of clear and drop it onto the top of each flower then I fill in with dump casing all over the bead.  important - the bead must be cool or you will smear the flowers but not cool enough to crack, also after heating the clear wait a second or so before you dump case so its just a touch cooler.

Then I do the ends again and heat the whole lot up and shape.  Let it cool and then I put it back in the back of the flame to flame polish ( I know this is done other ways but this is all I do).

Hope this helps and that I haven't forgotten anything.
:)
Title: Re: Spot encasing-tell me more
Post by: Mary on March 26, 2007, 03:22:51 PM
If you don't want to encase your vine, make encased stringers instead, using the opaques in the middle or covering those stripes with a transparent. It won't bleed as much. I prefer the depth of encasing the vines, but you can get round it.
Title: Re: Spot encasing-tell me more
Post by: Pam on March 26, 2007, 04:11:50 PM
Thanks Lesley, Manda amd Mary.
When i get home tonight I will post some pictures, I have achieved better results with flowers on top of encased vine etc but I always feel they are a liitle false looking, like Manda if I encase the vine then the flower i get whopping beads, also the flowers seem too big, my last batch -well you will see later some of the petals are lost or separated from the main part of the flower.
Also if I add the flower to the vine (not encased) i can only get 3/4 flowers and when finally encased the flowers are BIG, I want an abundance of dainty flowers without the bead being too big.
Title: Re: Spot encasing-tell me more
Post by: Pam on March 26, 2007, 05:38:25 PM
Here are my blooms that have upset me! Any advise is very welcome.
Title: Re: Spot encasing-tell me more
Post by: LesleyMac on March 26, 2007, 09:22:10 PM
I don't know how long you have been practicing these but they are not at all bad considering how difficult this is. I have to say I have made hundreds of flower beads much much worse than those.

Looking at them I would say the main problem is your bead is not cool enough when you are putting on the clear encasing causing some to smear, also I see what you mean about the depth on the first one, what if you tried just putting a smear of clear glass on top of the vines only, only problem though might be that it will end up misshapen.

I am no expert on encasing but from what I have read to get really thin encasing you have to heat up only the very end of the clear rod, very hot, but only the end and then swipe really quickly, it does take a lot of patience, everything about flowers takes patience though.  You have to be in for the long haul with flowers, you will find as you do more and more that you instinctively learn the heat levels.  I know its not a lot of help but its something you can't teach by telling I think you need to see someone actually doing it, maybe you should try to get on the Corinna floral course if you can afford it.

I also invested in some magnifiying glasses because you really need to get very small and its so difficult to see the detail.  Mine are just the clip on type that you can put over your own glasses if like me you are a bit shortsighted (my age you know).

Sorry I can't be more help but it will pay off if you persevere, I made loads and loads of failures but just kept going back to it, I am still no expert but thats mainly because whilst I love them I also like making other types so I am not totally obsessed.
Title: Re: Spot encasing-tell me more
Post by: glassworks on March 26, 2007, 09:28:18 PM
maybe kathy (my precious) will spot this - she is a demon at encasing, so much so we will be asking her to run sessions later in the summer!

;) 8)
Title: Re: Spot encasing-tell me more
Post by: Redhotsal on March 27, 2007, 12:21:07 AM
Hi Pam,
They're looking good to me, in fact. But you may find it easier if you make your florals very tiny. The encasing will magnify anything under there so you want to start off as small as you can. Most of my florals are made with stringer that is much less than 1mm diameter.
I'm a big fan of spot encasing as I find I put way too much clear on by the more "conventional" methods and I trap loads of air bubbles too 'cos I'm a bit slapdash. Make sure you have a very cool base bead and a very liquid/hot gather and you just "dot " the glass on. I even spot encase the vines too sometimes as I am a lazy so-and-so. But it works for me.
Title: Re: Spot encasing-tell me more
Post by: Redhotsal on March 27, 2007, 12:29:13 AM
Couple of other things I've remembered: Don't use anything remotely transparent as your flower base - yellow, red, stuff like that as they won't be "blocky" enough to show up the shape of the floral.

I use white and put a different transparent colour over the top. I love the corals and turquoises as they are alway very opaque.

Also don't get your base bead too hot when you melt the spots in to form the floral. Also don't blast them with a load of heat when you melt them in. Do it gradually and you will get a much better shape.
Title: Re: Spot encasing-tell me more
Post by: Pam on March 27, 2007, 08:44:10 AM
Thanks lesley for all the info and Sally, definately some things there that I need to pay attention to. Had another mini session last night, definately some improvement only problem was the clear bubbled loads, still the flowers were a wee bit better, I'll show you later after work.
Lesley when is Corina's floral course?
Title: Re: Spot encasing-tell me more
Post by: MangoBeads on March 27, 2007, 09:10:29 AM
Pam - just a thought are you nipping the end off your clear before you start- just melt in the flame and tweezer the end gets rid of tiny bubbles and scum !
Title: Re: Spot encasing-tell me more
Post by: Pam on March 27, 2007, 10:36:49 AM
Hi Manda, yes I did that, it may be there were inherent bubbles in the glass, which I shall look out for in the future. By the way great article in the Bead mag, wish I lived nearer you.
Title: Re: Spot encasing-tell me more
Post by: Pam on March 27, 2007, 06:08:04 PM
Pictures as promised(not very clear, sorry). I hadn't thought about a magnifying glass, I seem tohave trouble placing the dots, I hit the glass before I see it if you get what I mean. Do you think my dots need tobe closer together? The petal seem to float away from the centre.
Now moving on just a tad, how do I get a second layer of flowers (not petal) so I have say 6 or7 flowers in total on my bead without having a bead the size of a golf ball?
Title: Re: Spot encasing-tell me more
Post by: Mary on March 27, 2007, 06:57:38 PM
More layers need thin encasing, I'm afraid! And no, I can't do it right either! Looking good so far!
Title: Re: Spot encasing-tell me more
Post by: Redhotsal on March 27, 2007, 08:27:48 PM
Well Pam - they look better to me but I'd still go a lot smaller - I'm guessing the bead size is around 15mm? It's aesthetically nicer (I read this in a book but I can't remember whose) to see at least one and a half flowers in one "glimpse" of the bead so you need to make those babies small - or go for a bigger bead!
If you can manage to make them smaller then you'll find it much easier to spot encase - it will be just one big dollop over the floral. The slightly flattened shape at the end of the petals is where the encasing ends. Mine are often "truncated" in this manner - but if you can get the whole trio of dots in a space about 3mm across then you can cover it in one dollop. If the petals are starting to float off you need to plunge the centre of the trio much more. Don't be tempted to heat up the whole bead and do this - you need to heat just the group of petals only and really dig in with the pick. I use a stainless steel pick rather than a stringer. The pick will also push the dots together and it will give the floral a 3D shape. If you push hard enough (without actually pushing the bead off the mandrel!) you will be able to push the group of dots together even more which will make spot encasing a doddle. Can't speak for the super duper encasing artists on this forum as I am a real numpty spot encaser but if you want to have layers of florals then spot encasing is the way to go. Remember, you only need to encase the coloured bits (i.e. the petals) so you can keep the overall amount of clear glass down to a manageable size. I can fit at least three layers into an 18mm bead by spot encasing but you must keep those blooms small.
Hope this makes sense!
Sal
Title: Re: Spot encasing-tell me more
Post by: MyPrecious on March 27, 2007, 09:13:05 PM
Great advice everyone!! I've never managed to spot encase, I prefer encasing the whole bead.
For example, if it's a floral I'm making, here's how I do it:


I hope I explained everything ok, I'm not usually very good at that!
Title: Re: Spot encasing-tell me more
Post by: MyPrecious on March 27, 2007, 09:18:42 PM
I forgot to say that after melting in the flowers, I poke each one in the middle so a bubble forms when encased. But I'm sure you all know that! :)
Title: Re: Spot encasing-tell me more
Post by: Pam on March 28, 2007, 08:13:16 AM
Thanks you so much Sally and Kathy, I've got a day off today so guess what I'll be up to?
Title: Re: Spot encasing-tell me more
Post by: Pam on March 29, 2007, 07:01:12 PM
These are the results of yesterday, sorry about the poor quality of the photos, thank you Mary, Lesley, Sally and Kathy
Title: Re: Spot encasing-tell me more
Post by: Mary on March 29, 2007, 07:05:09 PM
Lovely Pam! The third one especially.
Title: Re: Spot encasing-tell me more
Post by: Redhotsal on March 29, 2007, 11:32:41 PM
Great work Pam - I like them all - and you have quite a few blooms in there (I can easily see over one and a half so you have passed the "aesthetic test" - lol!  :D)
They look pretty damn good to me - question is - are you happier with them, and what do you think made the most difference?
Beautiful beads though
Sal
Title: Re: Spot encasing-tell me more
Post by: Pam on March 30, 2007, 08:31:07 AM
Yes definately happier with them, I like the 2 smaller ones size wise. It was smaller dots for the petals that made the difference for sure with the spot encasing. The only thing with that was where the flowers are close together its difficult to be sure the whole of the opaque glass is covered. The smallest bead was encased with a wrap method (4 flowers), The largest has just 5 flowers but I think its a bit on the big side.
Thanks for you advise, I now feel I can progress with these techniques and produce beads to be proud of.
Title: Re: Spot encasing-tell me more
Post by: MyPrecious on March 30, 2007, 05:52:33 PM
Pam, those are great!!  :D
Title: Re: Spot encasing-tell me more
Post by: annasjewellerybox on March 30, 2007, 06:09:35 PM
those are lovely Pam,

and this is a fab thread, the next time i have torch time i am going to practice on my florals!!

;D
Title: Re: Spot encasing-tell me more
Post by: *rowanberry* on April 01, 2007, 09:48:20 PM
Those are lovely Pam! I couldnt do encased florals at all until I watched HP work and I got some tips :-) I only spot encase the flower, by doing a swoosh of very hot glass over a very cold bead only covering the flower. Works well for me!