Lampwork => Common Problems => Topic started by: helbels on November 25, 2009, 09:02:40 PM

Title: Sugar frit - what am I doing wrong?
Post by: helbels on November 25, 2009, 09:02:40 PM
Hello all

I managed to get hold of some very fine clear frit, to try to make some "sugar" beads with today.

I made my bead, rolled it in the frit while still glowing (to get it to stick) then removed and cooled it and put it in the fibre blanket. 

When I took it out - all the frit had gone!  Melted into the bead.. I assume melted by the residual heat from the bead as it's so fine.

I presume I am doing something very numpty-ish here, but I'm  not sure what....

Can anyone help?

Thank you! ;D
Title: Re: Sugar frit - what am I doing wrong?
Post by: Les on November 25, 2009, 09:05:23 PM
Maybe try letting your bead cool for longer once you've rounded it up ? Then just give the surface a sharp heat, then roll in frit ... there should be less heat in the core of the bead to radiate out toward the frit that way.... IFSWIM ??
xx