Technical Forum => Studio/workspace/setup/equipment => Tools and Presses => Topic started by: princess pink on September 10, 2009, 08:50:06 AM

Title: How to use a marble press??
Post by: princess pink on September 10, 2009, 08:50:06 AM
I just bought a marble press/ marver from maria, so only have the bottom half bit but although I've used one before it's not going so well. Can anyone offer some hints and tips please?

Thank you!  :-*
Title: Re: How to use a marble press??
Post by: Trudi on September 10, 2009, 09:01:27 AM
 make a barrel just a tinsiest bit shy of the edges - marver, add more glass to the ends so it looks like a dumbell - and melt in. The glass will naturally go to the middle. Keep gooing till you get there.
Title: Re: How to use a marble press??
Post by: Lush! on September 10, 2009, 09:28:31 AM
Haha, that's the opposite of how I do it, Trudi!

I just make a round bead and keep adding to the centre, then use the rim of the press to spread the glass to the edges.

How's that for confusing you Shahlaa?!!   ;D
Title: Re: How to use a marble press??
Post by: Trudi on September 10, 2009, 09:39:43 AM
I'll have to give your way a go Julie ............

I find by adding it at the edges it gives a dimpled hole. But always open to different ways!   ;)
Title: Re: How to use a marble press??
Post by: Lush! on September 10, 2009, 10:07:36 AM
... and I'll try your way!  :D
Title: Re: How to use a marble press??
Post by: Donna@Rockin' Beads on September 10, 2009, 10:27:19 AM
Oh bugger. It's no good, I'm going to have to get me a marble press. There's just way too much talk about marbles not to get involved!!!!
Title: Re: How to use a marble press??
Post by: Trudi on September 10, 2009, 10:43:54 AM
I use mine for round beads - not marbles!!
Title: Re: How to use a marble press??
Post by: hollergrafik on September 10, 2009, 10:47:31 AM
I couldnt do it til I tried Trudi's way, works reat for me now.
Title: Re: How to use a marble press??
Post by: Pat from Canvey on September 10, 2009, 11:12:08 AM
All this talk about marble presses so I've just given in and bought one from Maria Louisa.
Title: Re: How to use a marble press??
Post by: saffie on September 10, 2009, 12:43:29 PM
I was using my doming block yesterday to make round beads! Not to bad actually but PPP is needed!!!
Title: Re: How to use a marble press??
Post by: Donna@Rockin' Beads on September 10, 2009, 12:44:36 PM
Aha, I have one of those. Must give it a try.