I have decided to buy an Impress beadliner.
Is this the right silver tube to get for lining big hole beads?

http://www.cooksongold.com/Tube/Sterling-Silver-Tube-Ref-B-Outside-Diameter-6.0mm-Inside-Diameter-4.6mm-0.7mm-Wall-Thickness-prcode-RSA-020

Or should I get a smaller size?

Is there anything else I need to buy whilst I'm thinking about silver linning beads?
And, does anyone know of a copper tube supplier for beads?
Title: Re: Which silver tube should I buy.
Post by: Krysia@No98 on September 07, 2009, 02:37:29 PM
Copper, I haven't found one yet.  I have been looking as pumbing supplies.  Note though that 5mm is a very unusual size for copper pipe and with cost you two thirds to the same again.  I rang up one suppliers who said that they would email me with the details, they didn't and withdrew the product a few days later - humph!
Title: Re: Which silver tube should I buy.
Post by: hollergrafik on September 07, 2009, 02:56:58 PM
6mm microbore copper tubing looks about right for coring with copper. Its available in Wickes and places like that, comes in a roll so might be worth looking on ebay for shorter lengths.
Title: Re: Which silver tube should I buy.
Post by: Lush! on September 07, 2009, 07:11:16 PM
This etsy seller sells perfect silver and copper tubing, but she's away for a couple more days yet.

http://www.etsy.com/shop.php?user_id=5240805
Title: Re: Which silver tube should I buy.
Post by: dinah46 on September 08, 2009, 11:17:38 AM
Personally, I think that .7mm wall is too thick. You can get thinner wall tube from Rashbells even though it's not on their site, just ring them to see what they have.
Title: Re: Which silver tube should I buy.
Post by: Pandanimal on September 09, 2009, 09:25:21 AM
Thanks every one. I will have to see what I can find then
Title: Re: Which silver tube should I buy.
Post by: Pandanimal on September 09, 2009, 09:50:01 AM
Cooksons don't seem to have any other tubing that would fit on a pandora system as far as I can see.
I will have to try rashbells then.
The stuff on etsy looks good but would I have to pay import duty on it comming from the states?
Title: Re: Which silver tube should I buy.
Post by: Lush! on September 09, 2009, 09:53:42 AM
I don't remember paying any duty, its a small transaction.