I have turned on my new kiln today Paragon SC2. and I am following the instructions for the Ramp Hold practice programme and it is in F and the kiln was set in C so OH has changed it to F is that what most people use. I am getting more and more confused.
Edi
Title: Re: Kiln temperatures
Post by: mizgeorge on September 03, 2009, 02:19:34 PM
Hi Edi,
I think most of us here use C. There are some excellent schedules posted on the forum, and I think all of them are in C. I used to use Helen P's schedule for my SC2, and had no problems with it at all.
Title: Re: Kiln temperatures
Post by: Trudi on September 03, 2009, 02:23:13 PM
It's not really a problem which you use, but if you're asking questions or comparing what most people would do on here then °C is more useful for you!