 :o I made some silver glass beads - last night - ala Troll Lover Anouk's tutorial for silver glass...

I used a blue silver-glass very similar to Triton I think (was a freebie sample of short rods)

My question is - why are the beads even more colourfull tonight than they were this morning - seems like theres a lot more developed post annealing :-\ I dont get it ;)

Maz
Title: Re: Silver Glass - developing after annealing?
Post by: Trudi on September 04, 2009, 10:42:59 AM
Are you looking in a different light?
Title: Re: Silver Glass - developing after annealing?
Post by: mazmeabead on September 17, 2009, 08:43:38 PM
probably ;D
Title: Re: Silver Glass - developing after annealing?
Post by: Maikki on September 18, 2009, 09:40:24 AM
I was thinking the same, when I made a few basic encased beads from Ekho. At first they looked like amber with a little purple, but now they are more purple. But I thought also that it is probably light. We have had the most beautiful September here, sunny days with that special autumn light.