Fusing and Stained Glass Tips and FAQ's => Fusing Tips and FAQ's => Topic started by: bluefairy on August 22, 2009, 10:55:57 AM

Title: Can anyone help with this?
Post by: bluefairy on August 22, 2009, 10:55:57 AM
Ok, I made this bowl that I really like, made the blank, slumped it, THEN discovered this weird bubble, it looks like somehow a tiny bit of brass has got in.

(http://i357.photobucket.com/albums/oo15/helenbluefairy/P8220058.jpg)(http://i357.photobucket.com/albums/oo15/helenbluefairy/P8220059.jpg)

Anyone got any ideas how to fix it?  I thought of drilling it out, filling with clear powder and refusing, but don't think this will work coz I'd need to take it to full fuse temp to melt the powder, which would ruin the slump  :'(

Anyone got any ideas?
Title: Re: Can anyone help with this?
Post by: Zeldazog on August 22, 2009, 11:26:13 AM
Well, I suppose you could drill it out, re-fuse then re-slump....

Or, does it really detract from the piece, Helen - cos that looks fine to me!  Perhaps you could show us the whole piece.  Or send it to me for assessment....  ;D ;D
Title: Re: Can anyone help with this?
Post by: Sulis (Hazel) on August 22, 2009, 06:50:46 PM
Where is it on the actual bowl Helen? Is it slap bang in the middle, or off to the side? Is it really noticeable?

Is it too late to tack fuse some surface decoration onto it which could cover the spot and possibly re-slump if really necessary?

Or you could always sell it as a second if you're unhappy to let it go as it is? I'll bet most people wouldn't even notice it.

:-*
Title: Re: Can anyone help with this?
Post by: turnedlight on August 22, 2009, 08:42:38 PM
It's a lovely design - I don't know about fusing, but I don't think it's a big flaw, you could sell it as a slight second (people do love a bargain!) or keep it for a family pressie maybe? I'd think about just putting it out for sale and seeing what happens..
Title: Re: Can anyone help with this?
Post by: bluefairy on August 22, 2009, 10:52:03 PM
I think it probably is me being hyper wotsit about it, it just made me go "GAAAHHHHH!!!"  I'll take a piccie of the whole piece tomo so you can see what you think x
Title: Re: Can anyone help with this?
Post by: Zeldazog on August 22, 2009, 11:34:15 PM
Methinks Helen might be a perfectionist.....  ;)
Title: Re: Can anyone help with this?
Post by: bluefairy on August 23, 2009, 06:03:09 AM
Quote from: Zeldazog on August 22, 2009, 11:34:15 PM
Methinks Helen might be a perfectionist.....  ;)

Only in certain areas  ;)
Title: Re: Can anyone help with this?
Post by: Sulis (Hazel) on August 23, 2009, 08:38:38 AM
Quote from: bluefairy on August 23, 2009, 06:03:09 AM
Quote from: Zeldazog on August 22, 2009, 11:34:15 PM
Methinks Helen might be a perfectionist.....  ;)

Only in certain areas  ;)

Yeah - like everything glassy! We know, there is no escaping it. It's why your stuff is so damn GOOD!  :-*
Title: Re: Can anyone help with this?
Post by: bluefairy on August 23, 2009, 06:39:30 PM
fank you haze  :-*

Ok, excuse the shockingly bad photo, but here is the whole thing
(http://i357.photobucket.com/albums/oo15/helenbluefairy/P8230120.jpg)
Even though the pic is really bad, you can still see bad brassy bubble  >:(
Title: Re: Can anyone help with this?
Post by: beadysam on August 23, 2009, 07:41:59 PM
Sorry, no bright ideas except sell it as a second - or swap it on here, I'd certainly offer glass or frit as a swap if you fancied going down that route...? ;)
Title: Re: Can anyone help with this?
Post by: Hotglass28 on August 28, 2009, 12:36:23 AM
I think if you drilled it and placed a tiny piece of clear glass over the top (and I mean tiny) I think it might work.  BUT, you may get more bubbles forming from the sides of the hole you have just drilled because the drill bit is not very a very fine grade.

I would give it a go, or just sell it as a second or raise some cash for charity from the sale and put it down to experience.

Tis a bugger when this happens, glass has a mind of its own eh.

Denise- HTH
Title: Re: Can anyone help with this?
Post by: DragonflyLynne on August 28, 2009, 11:10:31 AM
I would sell it - I don't think it detracts from the bowl at all.  :)
Title: Re: Can anyone help with this?
Post by: sarah t on August 28, 2009, 11:17:21 AM
once it has stuff in it you would not see it ?...and imperfection is what makes it unique  ...
Title: Re: Can anyone help with this?
Post by: theflyingbedstead on August 28, 2009, 12:14:22 PM
I don't think that you need to sell it as a second...it is an interesting feature within the glass, and there are other bubbles there too.

Title: Re: Can anyone help with this?
Post by: bluefairy on September 01, 2009, 05:54:13 PM
I love the idea of selling it for charity, so i've decided to sell it for out Tommy's fundraiser.  Going to pop it in the Tommy's thread, but in the meantime, if you're interested, it's listed here
http://cgi.ebay.co.uk/ws/eBayISAPI.dll?ViewItem&item=160359732816 (http://cgi.ebay.co.uk/ws/eBayISAPI.dll?ViewItem&item=160359732816)

I hope someone wants it!  :-[