Lampwork => Lampworking Tip n Tricks => Topic started by: lemon kitten on August 04, 2009, 08:45:42 AM

Title: Frit stringer
Post by: lemon kitten on August 04, 2009, 08:45:42 AM
At the risk of sounding really thick.....(not difficult for me)  How can i make a stringer out of frit?  I'm assuming I dip a rod of clear in the frit, heat and pull but what if I want to make a stringer with striking glass??  Will it pre strike and will it be useable after?

Janey
Title: Re: Frit stringer
Post by: Dragonfire Glass on August 04, 2009, 10:42:48 AM
You can keep the stringer in a neutral flame until ready to to the business  :)
Title: Re: Frit stringer
Post by: Kaz on August 04, 2009, 10:53:39 AM
Is that called foreplay Colette :o :o :o
Title: Re: Frit stringer
Post by: GlassOcean on August 04, 2009, 10:55:24 AM
Quote from: Kaz on August 04, 2009, 10:53:39 AM
Is that called foreplay Colette :o :o :o

hahahahahaaaaaaaaaaaaaaaaaaaaaaa  :D ;D :D
Title: Re: Frit stringer
Post by: Mary on August 04, 2009, 11:07:22 AM
Sometimes pre-striking is an advantage, like with raku.

For pure frit stringers, heat a biggish bit and stick to the end of a big mandrel. Keep heating it and dipping in frit till you get a good sized blob to pull. Obviously a bigger grind is easier!
Title: Re: Frit stringer
Post by: Dragonfire Glass on August 04, 2009, 11:43:43 AM
Quote from: Kaz on August 04, 2009, 10:53:39 AM
Is that called foreplay Colette :o :o :o

;D  ;D well you can call it that Kaz  ;D  ;D
Title: Re: Frit stringer
Post by: Shirley on August 04, 2009, 11:58:39 AM
Quote from: Mary on August 04, 2009, 11:07:22 AM
Sometimes pre-striking is an advantage, like with raku.

For pure frit stringers, heat a biggish bit and stick to the end of a big mandrel. Keep heating it and dipping in frit till you get a good sized blob to pull. Obviously a bigger grind is easier!

This thread is sooooo wrong  :o  :D
Title: Re: Frit stringer
Post by: lemon kitten on August 05, 2009, 08:39:47 AM
Quote from: Shirley on August 04, 2009, 11:58:39 AM
Quote from: Mary on August 04, 2009, 11:07:22 AM
Sometimes pre-striking is an advantage, like with raku.

For pure frit stringers, heat a biggish bit and stick to the end of a big mandrel. Keep heating it and dipping in frit till you get a good sized blob to pull. Obviously a bigger grind is easier!

This thread is sooooo wrong  :o  :D

In EVERY way!

Janey x