I still have quite a lot of this can anyone tell me the best way to work it please ive had it since i first started and forgot about it came across it today .
xxcatxx
Title: Re: original Terra frit
Post by: turnedlight on July 23, 2009, 06:41:20 PM
Ooh you lucky, lucky..  ;D I would get a clear rod and coat the end in a few dips of terra, and make a thick stringer - terra is very easy, you just reduce a bit, and get lovely colours, or encase for muted lovely colours. It's great on ivory..
Title: Re: original Terra frit
Post by: catriona on July 23, 2009, 08:54:31 PM
Thanks thats great i,ll give that a try i,ve got about 50 grams of it so i,m going to have a great time .

xxcatxx
Title: Re: original Terra frit
Post by: Dragonfire Glass on July 23, 2009, 08:55:38 PM
Quote from: catriona on July 23, 2009, 08:54:31 PM
Thanks thats great i,ll give that a try i,ve got about 50 grams of it so i,m going to have a great time .

xxcatxx

If you'd like to send a gram or 2 my way, I can be very grateful  ;D
Title: Re: original Terra frit
Post by: beads-on-toast on July 23, 2009, 09:19:04 PM
i have Terra frit and it is fab
It reacts in a really aggressive way on Dark ivory and sits better with light ivory - if you work in with a marver i have found it produces purples and blues very easily