Post by: sparrow on July 19, 2009, 06:23:12 PM
Wasn't sure how to title this...my Paragon Caldera died after I did a PMC firing.....relay wouldn't click, it said thermocouple failure. We took it apart, put it back together...it was fine for 2-3 beadie sessions. This morning did a pmc firing, wanted to do beads tonight...lo' and behold, it's dead again. Hubby thinks it needs a new relay...any advice? it's about 18 months old...... :-\
Title: Re: Kiln dies after every PMC firing
Post by: Sarah on July 19, 2009, 06:48:33 PM
Hi Sabine

I would have a word with Rob at silverclay.co.uk - I found him very helpful whwn I had a problem with my SC2.

The only thing I can think is that there is something in your PMC cycle the kiln doesn't like - maybe it isn't coping with a high ramp speed for instance?

Hope you get it sorted

Sarah
Title: Re: Kiln dies after every PMC firing
Post by: sparrow on July 19, 2009, 07:02:13 PM
Thanks Sarah, we took it apart & put it back together again, and it's firing up happily again...I do ramp on 'full' for PMC, but I think other people ramp on 'full' for generic beadie sessions....? Anyways, we'll try a new relay, I'll try ramping a bit slower, and if that doesn't sort it, I'll call the cavalry  :)
Title: Re: Kiln dies after every PMC firing
Post by: ejralph on July 20, 2009, 07:47:13 AM
I think ramping full on to that temp is a little much for your Toasty.

When I do Art Clay firings, I tend to ramp up over an hour to the temp required and my caldera hasn't misbehaved at that.

Good luck and let us know how you get on

Emma
Title: Re: Kiln dies after every PMC firing
Post by: sparrow on July 20, 2009, 08:30:48 AM
Thanks Emma, I'll change it :)
Title: Re: Kiln dies after every PMC firing
Post by: Trudi on July 20, 2009, 08:39:19 AM
Got to admit - i tried to ramp my SC2 once on full and it just overshot!
Title: Re: Kiln dies after every PMC firing
Post by: ejralph on July 29, 2009, 11:40:59 AM
So, did it work ok on a slower ramp up?

Emma
Title: Re: Kiln dies after every PMC firing
Post by: Bluebottle on July 29, 2009, 11:56:17 AM
Quote from: sparrow on July 19, 2009, 07:02:13 PM
Thanks Sarah, we took it apart & put it back together again, and it's firing up happily again...I do ramp on 'full' for PMC, but I think other people ramp on 'full' for generic beadie sessions....? Anyways, we'll try a new relay, I'll try ramping a bit slower, and if that doesn't sort it, I'll call the cavalry  :)

Just a thought  :o is there an overheat trip built into  the kiln that would shut it off for a while   ???

Mike   ;D  ;D
Title: Re: Kiln dies after every PMC firing
Post by: sparrow on July 29, 2009, 11:58:41 AM
Not checked that Mike, thanks! And I haven't done a PMC firing since, so couldn't check the slow ramp (and am too lazy/scroogy to do a run with nought in't kiln)  ;D ;D
Title: Re: Kiln dies after every PMC firing
Post by: Dragonfire Glass on September 14, 2009, 06:11:34 PM
Did you sort the problem Sabine?
My kiln is displaying tlc which apparently is a problem with the thermocouple, either lag or failure.