Right chaps, sorry this has taken so long!!
This is the second colour challenge on Frit happens and it is
GREEN
You can make anythin that takes your fancy however the item must represent the main colour selected, which is green
A focal, a set a critter it is completely up to you.
We shall then award the winner with the winners avatar. You then have this avatar forever as they will be individual and dated
Sound good?
So lets go!!!
The next theme challenge will be started in May
Just posted mine all in the wrong place, so posting again
First one, ivory, gaia and silver plum
(http://www.lesleymcfarland.com/Beads20/IMG%5F3012%5Fedited%2D2%2Dmedium.jpg)
Second one a hollow, ivory and gaia
(http://www.lesleymcfarland.com/Beads20/IMG%5F3013%5Fedited%2D2%2Dmedium.jpg)
Third one ivory and green gaia focal
(http://www.lesleymcfarland.com/Beads20/IMG%5F3014%5Fedited%2D2%2Dmedium.jpg)
Heres a little bit of fun i was experimenting with last night
(http://i122.photobucket.com/albums/o262/beads-on-toast/paddyset.jpg)
oops forgot this one
(http://i122.photobucket.com/albums/o262/beads-on-toast/greenshell.jpg)
heres my little selection
green - kind of
(http://i122.photobucket.com/albums/o262/beads-on-toast/conkersorder2.jpg)
A few greens from me.
Kath
My green bead, inspired by my swap bead. Thanks Jim!
(http://i123.photobucket.com/albums/o297/weemaryanne/Mylampwork536.jpg)
Here's mine.... I'm still playing with frits.... some are better than others... there is a bit of devit on this one... but I think I'll etch it.. see if it improves.... I still love the colours.. just don't like the blemished surface ...
(http://i12.photobucket.com/albums/a230/lbrayford/greenentry.jpg)
Les xx
All your beads are absolutely wonderfull. I don't come even near your standard.
But here is my contribution (it is by the way my first creation and first bracelet) :
Well done to everyone - some stunning green efforts!!
Here's a couple from me, making steady but VERY slow progress (I've given up on encasing for now :-\)
I hope the pics are ok, it's a new camera & I'm sure I can get better results than this (reading the instructions would probably help ::))
Lovely beads Francoise, Les & Carol. You've all been much more creative than me! I struggle with green so decided to go for some stringer practice but as you can see I need more!
Fabulous work everyone!
Heres mine - I got addicted to raking and silver glasses as you may see...
Here's my offering - Nuggets of the Nile!
(http://i39.photobucket.com/albums/e160/shine-on2/Beads/nuggetsofthenile.jpg)
Thanks
Trudi
Here it is again.. LOL... but hey ! .. it's green :D
(http://i12.photobucket.com/albums/a230/lbrayford/oliveraku.jpg)
Here are my greens, I only managed three as a large spider ran across the desk and into my frit tray - I couldn't concentrate after that !