Lampwork => COE 104 => Topic started by: Jennie Lamb on July 03, 2009, 03:06:56 PM

Title: Annealing Bullseye and Dichroic
Post by: Jennie Lamb on July 03, 2009, 03:06:56 PM
Hello!  I am new to this game and am playing with different types of glass and have made some bullseye beads and decorated with dichroic.....Can I pop these into my bead cube and use the same program for annealing as I do for my other soft glass beads (the preset programme with an annealing temp of 520) or do I have to do something different?   I have read different opinions and would appreciate some advice.....Thank you x
Title: Re: Annealing Bullseye and Dichroic
Post by: Trudi on July 03, 2009, 03:16:06 PM
Quote from: jenniewren on July 03, 2009, 03:06:56 PM
Hello!  I am new to this game and am playing with different types of glass and have made some bullseye beads and decorated with dichroic.....Can I pop these into my bead cube and use the same program for annealing as I do for my other soft glass beads (the preset programme with an annealing temp of 520) or do I have to do something different?   I have read different opinions and would appreciate some advice.....Thank you x

i use the same and it's been fine for me!

BTW - I take it that dichroic was bullseye!
Title: Re: Annealing Bullseye and Dichroic
Post by: Jennie Lamb on July 03, 2009, 04:46:54 PM
Hi Trudi, A million thanks for that I was getting very confused  ???.  Yep the dichroic was bullseye....more by luck than judgement as it was only whilst I was browsing glass suppliers that I realised there was a difference, ho hum!

I am popping them in the kiln tonight and keeping my fingers crossed....thanks again for responding so quickly
Jennie
Title: Re: Annealing Bullseye and Dichroic
Post by: Trudi on July 03, 2009, 10:37:42 PM
No problem - - meant to add that  dichroic is only a coating  - it depends what glass it's on!!

And just so you know bullseye uses the same annealing schedule as 104!
Title: Re: Annealing Bullseye and Dichroic
Post by: Jennie Lamb on July 04, 2009, 02:27:48 PM
 ;) Hey Trudi, they survived and I am really chuffed with them thank you for the advice x
Title: Re: Annealing Bullseye and Dichroic
Post by: Trudi on July 04, 2009, 06:09:18 PM
Hope that you didn't hold your breath the whole time  :D   :D  :D

Glad that it helped - that's why we're all here!