I've just took delivery of a CIM sample pack and I'm finding it great to work with. I bulk anneal but I'm just hoping someone can confirm that I am oK to use the same timings/temperature as for effetre?
:)
Jo
Hi Jo, try this, taken from the Wiki above
Quotehttp://www.frit-happens.co.uk/wiki/CiM#Two_batch_annealing_schedules_for_CiM
Kirsty
Thanks Kirsty
Now where are the instructions for the kiln....off for a rummage
::)
what kiln have you got - someone may be able to help you out with a schedule ...
A trusty Paragon SC2
http://www.frit-happens.co.uk/forum/index.php?topic=859.0
here you go - good for 104 & 90 coe!
Aha, this is the one I am using anyway for Effetre, so that was my question really. If I use this will it be OK for CIM.
Also makes things simpler if I ever use 90coe although using a hothead I'm not sure I will ever have enough time on my hands to try to melt Bullseye !
Thanks Y'all
:)
Jo