Frit-Happens !

Lampwork => Common Problems => Topic started by: Zia on June 05, 2009, 05:47:45 PM

Title: another probably daft newbie question....bead cleaning tips and tricks
Post by: Zia on June 05, 2009, 05:47:45 PM
I am having serious problems cleaning my beads...

any good tips?

xxxx
Title: Re: another probably daft newbie question....bead cleaning tips and tricks
Post by: squirsygirl on June 05, 2009, 06:02:37 PM
I soak mine in warm water with a drop of liquid soap for an hour or so, and use a diamond reamer.  It makes a noise like fingernails on a blackboard - and I love it!

Kirsty
Title: Re: another probably daft newbie question....bead cleaning tips and tricks
Post by: Lloki on June 05, 2009, 06:09:29 PM
Quote[It makes a noise like fingernails on a blackboard - and I love it!/quote]
Weird!!!! :D :D :D
Title: Re: another probably daft newbie question....bead cleaning tips and tricks
Post by: Lloki on June 05, 2009, 06:11:17 PM
Brave attempt at being clever - LOL - OK back to my shed! :)
Title: Re: another probably daft newbie question....bead cleaning tips and tricks
Post by: Zia on June 05, 2009, 08:52:18 PM
thats what I have been doing and its awful!!!Especially on the smaller beads and the spacers

I was hoping there is a quicker and less annoying way ......

smiles

Title: Re: another probably daft newbie question....bead cleaning tips and tricks
Post by: squirsygirl on June 06, 2009, 08:20:00 AM
I find it quite relaxing. 

It's all a bit subversive, I wait till the others are all out, then I sit with a bowl of Hargen Daaz, and a bowl of warm soapy water, LOST onthe DVD player,

and I'm in heaven!

Kirsty
Title: Re: another probably daft newbie question....bead cleaning tips and tricks
Post by: Veebee on June 06, 2009, 05:27:54 PM
Cilit Bang and the bead release is gone! ( or so I hear...)

I use cola to soak my beads and a proper pipe cleaner from a tobacconist. Working a treat so far  ;D