Been torching this morning and I used what I thought was Dark Turquoise.
(http://i713.photobucket.com/albums/ww140/_Krysia_/th_P1010210.jpg) (http://s713.photobucket.com/albums/ww140/_Krysia_/?action=view¤t=P1010210.jpg)
It's got silver bits in it. It is dark turquoise or is it something else?
(scuse white stuff was practising stringer control, It was meant to be a straight line - no only kidding!)
I use a HH and bulk - almost of my coppery blues go a little silver.
I think it's a chemical reaction with the metals in the glass, and be really pretty.
Kirsty
yeah I'm on hh and Bulk too.
I thought it was pretty - just very suprised!
Ta
Krysia
It's reduced - the hothead doesn't have quite enough oxygen to keep the metal connected to its oxide. Metal oxides are in the glass to give the glass its colour. More oxygen = correct glass colour. Not enough oxygen = metally lustres.
Can be quite a nice look but it's also difficult to control with dk turquoise and a hothead. You can sometimes get rid of the grey/metally hue by soaking in Cillit Bang (Lime and Grime)
Hi Sal
Thank you
Sal, you are beginning to become 'Sal the Cillit Bang Gal'.!
I am - you'd think they were paying me a commission! :)
Sal - holding bottle of Cilit Bang ;D
Bang and the reduction comes right off ;DLOL
I also find that Jocks bead release remover rubbed on the bead takes it away .
xxcatxx
Really must try the Cillit Bang thing. Etching it does the job too. A 5 second dip will take off the reduction if it's slight. Or a full etch if it's heavy.
HP x
Quote from: catriona on May 23, 2009, 11:51:15 PM
I also find that Jocks bead release remover rubbed on the bead takes it away .
xxcatxx
how on earth did youfind that one out?? :D
Well you learn something every day. It doesn't always go grey, mine goes pink sometimes, sometimes it stays turquoise. It doesn't do it with light turquoise.
LOL i was cleaning bed release out of it and some got on bead i must have been rubbing as i turned the mandrel to clean inside when finished i noticed a patch where reduction rubbed away so got a clothdiped in pot rubbed bead allover and hey presto unblemished bead . ;D