I now have the means to make big hole beads and want to add silver cores........Do I fire the beads and then add the cores? Do I need something to add the cores? I have a look at Tuffnells but it dosent say how to add them :(
Ta
Michelle
If you run a search from the main index for silvercores, you should have quite a lot of info come up regarding tools required, machines you can use, tubing (size and annealing) and a DVD tutorial :)
You can get cores to simply push in (from Palmers metals, I think).
Marg x
Yeh... I think Tuffnells sell the glue in rivet ones too