Just got set up and started. Using a duel fuel with an oxycon.
Can someone tell me what I should do about bleeding my lines at the end of a working session. Or alternatively point me to an earlier thread that might have the information.
Thanks in advance.
Janet
This topic might help http://www.frit-happens.co.uk/forum/index.php?topic=12545.0;topicseen (http://www.frit-happens.co.uk/forum/index.php?topic=12545.0;topicseen)
Marg x
Thank you. Question answered.
Janet