Morning Ladies and Gents,
I have this afternoon off to have a play and try and figure out where I am going wrong. I am now actually producing round beads, however when you look at their side profile you can see that they have have a slight tear drop shap to them.
Any ideas on what I am doing wrong? Is my first layer of glass not even enough, am I not spending enough time shaping the bead?
Its driving me nuts :(
Any help would be brill
Sounds like your mandrel is slightly off horizontal when you are shaping?
yep... what Sooz said.
Try drawing a horizontal line just behind your torch to act as a guide when you are shaping :)
Quote from: Les on April 21, 2009, 11:22:44 AM
yep... what Sooz said.
Try drawing a horizontal line just behind your torch to act as a guide when you are shaping :)
What a good tip Les am gonna try that cos I am pants at making round beads ;D
So its not so important when I am applying the glass, only when I am shaping it?
A lot of people shape as they go, I just blob lumps on and shape later :)
Quote from: Soozintheshed on April 21, 2009, 11:45:30 AM
...I just blob lumps on and shape later :)
too much technical speak on this forum ;D
All my beads used to have a lovely dimple on one end and grotty hole on the other ??? I just learned to keep an eye on the angle I was holding the mandrel :)
when i spent my day with julie ...my beads were not a bad shape till i tried to check what shape they were :(.......maybe a mirror to check rather than moving the mandrel ...but i guess really its just practise and knowing glass better
and using a marver to make it look deliberate !!!
i quiet like lemon pip shaped beads if its any concellation lol