Frit-Happens !

Lampwork => Common Problems => Topic started by: Sarah999 on April 17, 2009, 12:24:21 AM

Title: Bad Beads...
Post by: Sarah999 on April 17, 2009, 12:24:21 AM
Hi. Just a quickie.

I just made a delicious bead, BUT then I decided to poke holes in it and encase it in clear - which ruined the bead.
So I was wondering is it possible to smash it up and use it as frit? or will it not melt properly?

Also... I have been taking my beads off their mandrels, but was going to send them to someone to anneal them. Should I be leaving them on the mandrels to do?

Thank you

Sarah
xxx
Title: Re: Bad Beads...
Post by: sarah t on April 17, 2009, 12:30:28 AM
better luck next time hun  :(
Title: Re: Bad Beads...
Post by: hollergrafik on April 17, 2009, 12:31:49 AM
If you smash it for frit you will have to get every tiny scrap of bead realease off or it will show in the bead you add the frit to, add it to ya fugly pile, this pile will get BIG believe me LOL. I got some of the beads I made last year out recently and laughed my arms off.
Title: Re: Bad Beads...
Post by: Sarah999 on April 17, 2009, 12:33:45 AM
Hmmm I was wondering about this.
Good point. The colours are just so delish though. I might have to make some frit with these colours anyway.

xxx
Title: Re: Bad Beads...
Post by: Lush! on April 17, 2009, 08:13:59 AM
Quote from: hollergrafik on April 17, 2009, 12:31:49 AM
laughed my arms off.

:o :o

That could make lampworking rather difficult ...
Title: Re: Bad Beads...
Post by: princess pink on April 17, 2009, 09:52:19 AM
oh dear...another one for the fugly pile me thinks! lol!

no take em off the mandrels to post for annealing but don't clean em til after x
Title: Re: Bad Beads...
Post by: Sarah999 on April 17, 2009, 11:43:22 AM
I have cleaned some of them. But not very well.
Should I try and re bead relese them?
:S

xxx
Title: Re: Bad Beads...
Post by: Steampunkglass on April 17, 2009, 11:58:00 AM
I wouldn't personally, they should be ok as they are, I've batch annealed with and without bead release. I used to end up cracking or chipping them by cleaning them before I annealed them