Lampwork => Lampworking Tip n Tricks => Topic started by: beads-on-toast on March 31, 2009, 10:16:21 PM

Title: goldstone chips - can you melt them?
Post by: beads-on-toast on March 31, 2009, 10:16:21 PM
Hi Guys,

On the arrival of Sarah's new E-book, just wondered, can you melt the goldstone chips which have a hole running through?

They're rounded off in shape but are they the same thing? not resin-y?
Title: Re: goldstone chips - can you melt them?
Post by: Cecilia on March 31, 2009, 11:16:06 PM
i used some goldstone beads to make stringer with. i heated them and dropped them in water so they shattered and them melted them into transparent. probably not the correct thing to do but it worked ok and nothing cracked but only put it on the surface.
try it, why not, see what happens...

Cecilia X
Title: Re: goldstone chips - can you melt them?
Post by: Ilona on March 31, 2009, 11:18:32 PM
I had a string of goldstone , and I have melted them and used them as encased stringers, no problem.

I have just run out and ordered a chunk tonight.
Title: Re: goldstone chips - can you melt them?
Post by: Vicki on April 01, 2009, 12:32:19 AM
I had some blue goldstone beads & I put them in a bag & hit them with a rock....they melted & sparkled, but I felt a bit mean afterwards  :D
Title: Re: goldstone chips - can you melt them?
Post by: Trudi on April 01, 2009, 08:10:47 AM
Quote from: Vicki on April 01, 2009, 12:32:19 AM
I had some blue goldstone beads & I put them in a bag & hit them with a rock....they melted & sparkled, but I felt a bit mean afterwards  :D

Bead basher - I should report you to the bead police!!!  :o
Title: Re: goldstone chips - can you melt them?
Post by: lemon kitten on April 02, 2009, 06:11:49 PM
I bashed my block of goldstone into little lumps....encased them in clear and pulled into stringers.  MUCH better than the pre-made stringers the goldstone was MUCH more obvious.

Janey x
Title: Re: goldstone chips - can you melt them?
Post by: Carol on April 02, 2009, 06:54:13 PM
Ooh I've got quite a lot of goldstone beads in a box somewhere. Think I'll dig them out & try bashing them with the hammer   ;) Thanks for the tip  :)
Title: Re: goldstone chips - can you melt them?
Post by: Mary on April 02, 2009, 06:54:56 PM
I've done it too! Only thing is you don't know the coe (it's glass and copper). I've seen 96, Bullseye 90, and 104 for sale for beadmakers, at least you don't need to worry what you can use it with.