Frit-Happens !

Tutorials in here.. => Lampworking => Sculptural => Topic started by: StudioMarcy on March 26, 2009, 03:39:36 PM

Title: Mini Tutorial on my blog- Making Sculptural Mushrooms
Post by: StudioMarcy on March 26, 2009, 03:39:36 PM
Hi everyone,
I just added a mini tutorial on my daily glass blog today. (http://www.StudioMarcy.blogspot.com)

It's how to make little mushrooms- you know, fairy garden types.  Please feel free to visit if you have a spare minute.

Here's the exact url: http://studiomarcy.blogspot.com/2009/03/mini-tutorial-making-mushrooms-by-marcy.html

Hope your day is going well.
Take care,
Marcy

http://www.StudioMarcy.etsy.com
Title: Re: Mini Tutorial on my blog- Making Sculptural Mushrooms
Post by: Paula on March 26, 2009, 04:38:17 PM
Marcy, a lovely tutorial.
Very easy to follow, and any tut that instructs you to pat yourself on the back, is always going to be a winner with me!
Title: Re: Mini Tutorial on my blog- Making Sculptural Mushrooms
Post by: greenbeadenvy on March 26, 2009, 07:06:22 PM
Awww they are cute! I may have a go tomorrow if I get time.
I also love your Langston Puppy but then I would, I lurves dog beads ;D
Title: Re: Mini Tutorial on my blog- Making Sculptural Mushrooms
Post by: Revontulet on March 26, 2009, 08:46:57 PM
Very clear tutorial, Marcy - & cute mushrooms! Thanks for sharing  ;D
Title: Re: Mini Tutorial on my blog- Making Sculptural Mushrooms
Post by: StudioMarcy on March 30, 2009, 09:17:27 PM
Thank you.  It's simple and kind of fun.

Marcy
Title: Re: Mini Tutorial on my blog- Making Sculptural Mushrooms
Post by: sarah t on March 30, 2009, 09:28:53 PM
as a newbi im amazed who is here !!!.......i bought a  baby dragon from you a month or so ago from etsy ...it was a pressie for someone and she just loved it .....(http://i304.photobucket.com/albums/nn173/thomo1962/011.jpg)

Title: Re: Mini Tutorial on my blog- Making Sculptural Mushrooms
Post by: StudioMarcy on March 31, 2009, 01:33:53 AM
Well hello.  I'm so glad your friend likes her.  Baby dragons are one of my favorite beads to make.

Thanks for the photo too.
take care,
Marcy
Title: Re: Mini Tutorial on my blog- Making Sculptural Mushrooms
Post by: julieHB on March 31, 2009, 08:16:49 AM
Aaaw, she's so cute!!