I'm still a relative newbie, been going almost a year but still feel VERY much an amateur.  I've just been looking at some lovely colours in the Bullseye range and discovered that Bullseye is 90 coe.  I work on a hothead torch, would Bullseye work well in a HH flame? I've only used 104 Effetre, CIM and TAG (Tibet)(which turned out like poo on a stick :-[) so far.

Expert advice would be much apprecited. Thanks. 8)
Title: Re: Bullseye on HH?
Post by: turnedlight on March 06, 2009, 06:16:55 PM
I've done it in the past..
Title: Re: Bullseye on HH?
Post by: garishglobes on March 06, 2009, 07:17:02 PM
I have too. I don't think it is a problem, because although the COE is slightly less, Bullseye make the glass a bit more workable to make up for it. I love Bullseye - the colours are gorgeous and the glass is just that little bit easier to manage, somehow, than some of the 104 COE. It just seems to work nicely. :)
Title: Re: Bullseye on HH?
Post by: Scubeadoo on March 06, 2009, 09:42:29 PM
I started with this using an old glassworking torch that my husband was given years ago, it works pretty well with a hothead and there are some lovely pinks and purples in the range.
The Lustre rods are fun too - using my old torch which has a reducing flame I can get the blue lustre to look like haemetite.
Title: Re: Bullseye on HH?
Post by: Flyingcheesetoastie on March 06, 2009, 09:47:05 PM
I've generally found Bullseye to be slower working on a hothead due to it being a harder glass, but I wanted to query the TAG glass too, isn't that borosilicate?  If that's the case, then I doubt a hothead is getting hot enough to do anything but turn it to poo!
Title: Re: Bullseye on HH?
Post by: garishglobes on March 06, 2009, 11:05:34 PM
TAG do 104 COE as well as borosilicate - though I would think that, like other silver-rich 104COE glasses, the reducing ones would work better on a HH than the strikers.
Title: Re: Bullseye on HH?
Post by: Mand on March 07, 2009, 02:22:21 PM
It was 104 TAG I used. I only bought a couple of rods and just didn't like it.  :P

I love pinks and purples too which was what drew me to the Bullseye, but if you say it can be slow I may give it a miss as I really hate slow glass on my HH, it takes soooooo long to work into something usable.
:-\
Title: Re: Bullseye on HH?
Post by: soulsilver on May 19, 2009, 12:53:12 PM
Hi There, I am on a hothead and I have been using TAG silvered glass, its great, I am completely in love with Taxco silver turquoise, lake geneva and deep purple, I have only been working with the hothead for about 8 weeks, these are some of the beads I have made using TAG

(http://i209.photobucket.com/albums/bb144/Sals25/DSCF7699.jpg)

Deep Purple

(http://i209.photobucket.com/albums/bb144/Sals25/DSCF7682.jpg)
Taxco silver turquoise

I got some great advice on how to work with this glass from Sean at Off-Mandrel, also if you look at the glass descriptions on his site it tells you how best to work the glass, I made a note of this and kept it beside me ( I have a shocking memory!)

HTH

Sally
Title: Re: Bullseye on HH?
Post by: Trudi on May 19, 2009, 02:13:41 PM
Although I'm using a minor I find that most of the BE glass melts just as easy.
Title: Re: Bullseye on HH?
Post by: Lloki on May 19, 2009, 05:26:23 PM
I've used BE on a HH  - it can be done (just takes a little bit longer)

Soulsilver - love your beads, especially the deep purple one - yummy ;D