Frit-Happens !

Lampwork => Common Problems => Topic started by: turquoise on February 22, 2009, 04:17:57 PM

Title: Making barrel beads
Post by: turquoise on February 22, 2009, 04:17:57 PM
Hi I am really loving the barrel shaped bead at the mo and wondered if anyone had any useful hints for making them. Or if there is a tutorial which would help me out?

Thanks
Vicky
Title: Re: Making barrel beads
Post by: sparrow on February 22, 2009, 05:30:49 PM
I love using a lentil base as a marver ;)
Title: Re: Making barrel beads
Post by: garishglobes on February 22, 2009, 06:48:24 PM
Or you could make a bicone, flatten the middle ridge slightly and then add heat to round off :)
Title: Re: Making barrel beads
Post by: clasicat on February 22, 2009, 06:53:00 PM
Get a Tube shaper this is my fav shape of bead and the one I make most often and I use my tube shaper all the time
http://www.cattwalk.com/formingtrays.htm#Tube%20Shaper
Title: Re: Making barrel beads
Post by: Pat from Canvey on February 22, 2009, 07:48:20 PM
If by barrel you mean beer barrel, then a spoon will give you a reasonable shape. Put your mandrel accross  the spoon and rotate. The bowl will shape the bead provided you keep the mandrel touching the sides of the bowl. Use the size of spoon that fits the size of bead you want to make. I'm all in favour of using kitchen items to shape glass. A cheese grater makes a great pattern on plain beads.  ;D  ;D
Title: Re: Making barrel beads
Post by: Kaylee on February 23, 2009, 08:45:03 PM
Quote from: clasicat on February 22, 2009, 06:53:00 PM
Get a Tube shaper this is my fav shape of bead and the one I make most often and I use my tube shaper all the time
http://www.cattwalk.com/formingtrays.htm#Tube%20Shaper

Clasicat thanks for this, didn't know it existed - and I love this style of bead, couldn't figure out how to do it...

but now I'm blaming you  ;)  I have just bought it and a press as well!!!  Oops finger slipped.  Honest. Oh well too late now  ;D
Title: Re: Making barrel beads
Post by: TiaraHelen on February 23, 2009, 08:56:50 PM
Wow that tube shaper looks great - but I'm thinking tax, import duty, handling charges, falling exchange rate, OUCH! Don't suppose there's a change anyone has got one they don't want?:D
Title: Re: Making barrel beads
Post by: beadysam on February 23, 2009, 09:04:21 PM
This any good?
http://cgi.ebay.co.uk/Bead-Press-Barrel-Bi-Cone-FormTool-Bi-Cone-Mold_W0QQitemZ150327566130QQcmdZViewItemQQptZLH_DefaultDomain_0?hash=item150327566130&_trksid=p3911.c0.m14&_trkparms=72%3A1229%7C66%3A2%7C65%3A12%7C39%3A1%7C240%3A1318
Title: Re: Making barrel beads
Post by: TiaraHelen on February 23, 2009, 09:12:01 PM
Thanks Sam!
Title: Re: Making barrel beads
Post by: garishglobes on February 23, 2009, 09:15:58 PM
I got mine from him - he's great, lovely guy and its unlikely to get stung for customs at that price. :)
Title: Re: Making barrel beads
Post by: TiaraHelen on February 23, 2009, 09:41:09 PM
Thanks for the tip, I've messaged him to check postage...
Title: Re: Making barrel beads
Post by: beadysam on February 24, 2009, 10:19:31 AM
His P&P is usually reasonable, and although I've bought a few things from him, only once have I been caught by customs. ;)
Title: Re: Making barrel beads
Post by: TiaraHelen on February 24, 2009, 10:21:02 AM
bother, I bought it, how did that happen?
Title: Re: Making barrel beads
Post by: mel on February 24, 2009, 01:25:07 PM
I make squat little barrels by making a biggish round bead, then marvering lightly and evenly at the waist which will elongate the bead slightly, then I gently heat the waist so it just rises up in a slight curve.
Title: Re: Making barrel beads
Post by: beadysam on February 25, 2009, 02:18:30 PM
Quote from: TiaraHelen on February 24, 2009, 10:21:02 AM
bother, I bought it, how did that happen?

I know, isn't it strange?  Things like that keep happening to me too - must be some sort of lampworkers curse! :o