Frit-Happens !

Lampwork => Lampworking Tip n Tricks => Topic started by: GlassOcean on February 13, 2009, 05:20:23 PM

Title: Etching question.
Post by: GlassOcean on February 13, 2009, 05:20:23 PM
Hi Lovelies,

I am itching to try etching!  The only thing I can find on ebay is Armour Etch glass cream, is this the right stuff?  Is it any good?  If not where can I get the right stuff?

http://cgi.ebay.com/Armour-Etch-GLASS-ETCHING-CREAM-22-Oz-New-Improved_W0QQitemZ380103166611QQcategoryZ3099QQcmdZViewItemQQ_trksidZp3907.m221QQ_trkparmsZalgo%3DDLSKWL%26its%3DK%26itu%3DMBMS%252BUCK%26otn%3D34%26ps%3D48 (http://cgi.ebay.com/Armour-Etch-GLASS-ETCHING-CREAM-22-Oz-New-Improved_W0QQitemZ380103166611QQcategoryZ3099QQcmdZViewItemQQ_trksidZp3907.m221QQ_trkparmsZalgo%3DDLSKWL%26its%3DK%26itu%3DMBMS%252BUCK%26otn%3D34%26ps%3D48)

Thank you thank you thank you

:-*
Title: Re: Etching question.
Post by: sparrow on February 13, 2009, 05:23:53 PM
Get the liquid from Martin, Kerensa, I'm trying for a link, but if it doesn't work, it lives on the second or third page of 'Bead Making Equipment' :)

http://www.tuffnellglass.com/index.html?lang=en-uk&target=d28.html
Title: Re: Etching question.
Post by: Lush! on February 13, 2009, 05:25:46 PM
Sabine beat me!  I was trying to get the link too  ;D
Title: Re: Etching question.
Post by: GlassOcean on February 13, 2009, 05:30:09 PM
Thanks you lovely 2!

>..........scuttles off to martins!