Ok - I should maybe know the answer to this - but what size bead hole do you get with a 2.4 mandrels?
Thanks in advance :D
A bit bigger than 2.4mm, depending on the thickness of the bead release used. Not meant facetiously, by the way ;)
I have always wondered that too. I see on some websites that the beads have a 2mm hole, and presumed that they'd used 1.6 mandrels, but am I wrong? Is there a 2mm mandrel as well?
:)
I think ppl list the size of the mandrel and not the actual size of the hole. I use 2.4mm mandrels so I say 2.4mm (although I originally thought they were 2mm!!)
As Shirley says, the thickness of the bead release can make a huge difference.. especially for someone like me who double dips!
And, yes, I've seen 2mm mandrels for sale before :)
x
dinah46 sells 2mm mandrels on her website. I find them ideal as they are not too thick for most presses but not as prone to bending as the 1.6mm and a nice size for doing spacers too.
Kazx
thanks for that, will have a look. I sometimes find the 2.4mm a little large for what I want, but like you say Kaz the 1.6 can be a little bendy. I even had one bend on me in the flame the other day! ;D
Thanks for the plug Kaz :D
Yep I have some 2mm mandrels on my website :)
thanks guys - I saw on a bead makers web site that a 1/6 mandrel has a 2mm bead hole - I'll have a look a the 2mm mandrels too :D
Quote from: Kaz on February 08, 2009, 09:45:13 PM
dinah46 sells 2mm mandrels on her website. I find them ideal as they are not too thick for most presses but not as prone to bending as the 1.6mm and a nice size for doing spacers too.
Kazx
I've just seen these (not from this post) - and bought some to try! as I find the same thing!
I usually give the size of the mandrel the bead was made on and then indicate the likely hole size as a bit bigger - I use a 1.8mm mandrel (I think - its thicker than a 1.6 and def. thinner than 2) so expect the hole to be nearer 2mm by the time I've allowed for bead release and cleaning.
Quote from: ebj on February 08, 2009, 09:03:25 PM
Ok - I should maybe know the answer to this - but what size bead hole do you get with a 2.4 mandrels?
Thanks in advance :D
just measured one with my digital thingy (technical term ;)) and they are 2.8mm but it dose depend on your bead release
lol - like your term caroline :D Need to get me a digital thingy :D
its right up there with a what-ya-mac-call-it and you-know-what-i-mean-that-thing-there (the later is to be done whilw waving your arm in the direction of what you mean) ;) ;D
Apparently digital calipers at Lidl in the next week.. I'm getting one!
http://www.lidl.co.uk/uk/home.nsf/pages/c.o.20090216.index.ar6
Quote from: turnedlight on February 09, 2009, 05:45:54 PM
Apparently digital calipers at Lidl in the next week.. I'm getting one!
http://www.lidl.co.uk/uk/home.nsf/pages/c.o.20090216.index.ar6
mine are from Lidi i think, or was it Aldi, only cost £8ish (ish is also a technical term, just incase you where wondering) I wouldn't be without mine now
Lidl have bolt cutters too for £6.80. Great for cutting down mandrels.
http://www.lidl.co.uk/uk/home.nsf/pages/c.o.20090216.p.Bolt_Cutters.ar4 (http://www.lidl.co.uk/uk/home.nsf/pages/c.o.20090216.p.Bolt_Cutters.ar4)