Frit-Happens !

Lampwork => Common Problems => Topic started by: Jivesjools on January 22, 2009, 11:41:56 AM

Title: Fibre blanket
Post by: Jivesjools on January 22, 2009, 11:41:56 AM
How long do i need to leave the beads in the fibre blanket to cool?

Thanks

Rach
Title: Re: Fibre blanket
Post by: Carol on January 22, 2009, 11:46:25 AM
Till you can pick them up without burning your fingers!  ;D
Title: Re: Fibre blanket
Post by: Kaz on January 22, 2009, 11:48:13 AM
Possibly up to an hour to ensure that they don't crack - some people may recommend longer but personally I like to have a peep well before that!!!