I`ve just found that Warm glass are stocking Mica Powder and got all excited because I`ve wanted to use it for ages. What colours are best to use? I don`t want to part with my cash and find I`ve spent it on a crappy colour that won`t give results. any advice glady received. Thanks guys! :)
Glad you asked about mica powder Rachel, I noticed it on Warm Glass site.
What do you actually do with it, how is it used? I only fuse, so wonder if/how I could use it?
Cos, its not like I haven't got tons of stuff already.....
I lurve mica powder!
I bought a huge sample pack (either 24 colours for £16 or 16 colours for £24!) ages ago but I find them hard to use - I like the bigger pots cos I can literally dip my bead in, give it a twirl in the powder, tap off the excess, briefly reheat the bead to stick the powder on, then into the kiln.
I've got gold and pearl in the bigger pots and I just added a pic of some gold-dusted beads to my Flickr album today.
Quote from: Zeldazog on January 19, 2009, 04:15:03 PM
Cos, its not like I haven't got tons of stuff already.....
You can never have enough stuff.......... ;)
I think for fusing you can sprinkle it on glass/sandwich it between sheets, I'm guessing maybe beads can be rolled in it?!?!? ??? Never tried it though (as you can probably tell). It's on my (v long) to do list...........
Oooooo, thank Julie and Dawn! I`m gonna have a nosey at your bead now and may have to get myself some to play with!
I found that colour really depends on what colour glass you go over. Red pearl over red was very pink and striking for example, I have some green and blue which tends to look pretty good although I haven't used it for a while.
Doesn't seem to work very well inside glass, I found it didn't show up much, but on the outside worked a treat.
I actually used to use it over gold ormaline paint rather than glass, and I remember the contrast between cold blue and warm gold was quite striking
This brings up a question from me. ;D
When I asked Tuffnells if they sold this at the Big Bead show at Sandown, they said a definite no. It was apparently dangerous to use ??? If I'm correct the manufacturer would not disclose the contents so Tuffnells would not buy it in. I hope I've got that right :)
I haven't looked into it any further but is there some safety procedures with it? Does anyone know of issues with using it. Would be grateful to know as I love the effect. I have drooled over yours in the past Julie ;)
Thanks guys ;D
Im no expert on the stuff, but just take the same care as you do with enamels, Ie, dont breath, inhale or sniff!
And a little goes a VERY long way!
I've used it very sucessfully in fusing projects, but with fusing you do need to use quite a bit to get a good result!
I think the sparkle colours are better than the glitter or hi-light ones, but thats just me!
Quote from: Lush! on January 19, 2009, 04:20:30 PM
I lurve mica powder!
I bought a huge sample pack (either 24 colours for £16 or 16 colours for £24!) ages ago but I find them hard to use - I like the bigger pots cos I can literally dip my bead in, give it a twirl in the powder, tap off the excess, briefly reheat the bead to stick the powder on, then into the kiln.
I've got gold and pearl in the bigger pots and I just added a pic of some gold-dusted beads to my Flickr album today.
Aha I was just gonna pm up about the beads you put on UK beaders in the gold thread to see how you achieved the look and now I know ty ;D
The mica is the same stuff they use in eyeshadow, so it's not as bad as enamel, just be sensible.
Those purple sparklies are gorgeous, Christina!
Mary, does that mean we can use loose eyeshadow instead, then?
Marg x
It's tempting, but I think they add alot of other fillers and stuff in with it as well
Some colours of Pearl-ex work, but some burn out, I imagine eyeshadow is the same. The mica is fine, but the dyes and colourants don't tolerate the heat.
Hiya Guys, I was looking on etsy the other day and came across this Pink Tint Sparkle Bead Set by joycelo. http://www.etsy.com/view_listing.php?listing_id=23906039 (http://www.etsy.com/view_listing.php?listing_id=23906039)
(http://i644.photobucket.com/albums/uu164/vickiwhte/il_430xN66891847.jpg)
Can anyone tell me how this person has created this glitter look, she says she rolled it in sparkling dust to create an all over shimmer??? and any idea where I can get my hand on some .... ;D
Thanks ;)
xxx
Warm Glass sell a range of colours. I got very tempted!
Quote from: theflyingbedstead on April 30, 2009, 08:44:28 AM
Warm Glass sell a range of colours. I got very tempted!
Warm Glass?? (I'm very new to lampworking but obviously I'm hooked!!!!) sell a range of colour of what? I'm terrible arn't I!!!! x
Hi, Pippa from Warm Glass here. We stock the Mica powders in three effects : sparkle, highlight and glitter depending upon the effect you want to achieve. I have copied below, the advice given on our suppliers website which hopefully will be of interest:
For Fusing/Slumping:
Usually only used by the glass beadmakers, this is an attractive product that can be used on fused glass pieces to great effect. The metallic colors add highlights to a piece at minimal cost. There are several ways to use this powder. It is suitable for use on any type of glass, both soft and float. If you want to make it into a paint consistency, it needs to be mixed with a water based medium, such as Klyr Fire or Water Friendly Medium, and water, till desired consistency for technique being used. This mixture should be dense enough to have a good layer adhering to the glass before firing. Use plenty of the medium, as this is what helps to 'stick' the powder to the glass when it dries. The rule of thumb is "what you see is what you get". Test your mixture on a scrap of glass and let it dry. If the color is very pale, add more powder to the mix. If it dries very dull and 'scummy' looking, thin down a touch. Fire the piece to fusing temperature to get the powder to 'stick.' This is an inert material, and only what is in direct contact with the glass surface will stay on after firing, the rest will brush away. This is why a good mixture needs to be made with the painting medium to help this process. It is also fine for air-brushing onto the front OR back of the glass. Being inert, it will NOT stick to the kiln wash on the shelf or mould! Mix with the medium till correct consistency for spraying. On the top surface of the glass, it leaves a soft semi matt metallic coating, on the back a subtle "mirror" like effect, depending on the color. Once again, dust off what does not adhere in the firing process, and store for re-use. If you want to paint a design between 2 pieces of glass, care should be taken to make sure there is still enough unpainted glass to fuse to the base glass. The powder acts as a separator, and prevents the 2 layers from fusing if coated all over. Remember to burn off the paint medium before placing the 2 pieces together! Gases from the burning off could be trapped between the layers if this is not done. The powder can also be sprinkled onto the glass, but again, only what is touching the surface will stick, dust the rest off after firing for using again. Hair spray can be used to help the powder stick while you are working on the decoration. It can also be mixed with clear enamel powders or powdered frit and sifted over the glass. It is advisable to test the different colors first to make sure you get the results you are looking for.
For Beadmaking:
Use Mica Powder to create a sparkle or pearl luster color inside glass or on its surface.
To use, form glass to its final shape. Allow the glass to harden but, still remain hot. Quickly heat the surface of the glass until molten. Avoid allowing the inside of the glass to become molten or it will probably loose its shape during some of the following application methods. Any of the following methods can be used to apply Mica powder. Pile Mica Powder onto a metal or graphite work surface. Dip the glass into the powder and rotate it around until the glass is covered. The powder will only permanently adhere to molten glass. If you find that the powder did not adhere to the glass, it was not hot enough. The glass will coat with a thick layer of powder, but only the layer of powder that is in actual contact with the molten glass will adhere. The rest will be loose. Put the glass back into the flame to flame anneal it. Only use the cool end of the flame or the powder will burn onto the surface of the glass and the item will probably be ruined. Another application method is to place the powder into a small metal bowl or cup. Apply the powder by inserting the glass into the bowl. Because Mica Powder is made of mica, it is an excellent insulator. While the glass is engulfed in the powder, it performs a pseudo kind of flame annealing. You can also apply the powder by sprinkling or sifting it onto the glass. An enamel sifter works well. Sprinkling or sifting is the best method when you only have a small amount of powder to work with.
To encase glass that has just been coated, wipe off excess layers of powder first. Use a dry cotton cloth and wipe with a quick motion. Be careful with how you handle the cloth and where you put it, because it will get very hot and may catch fire. If you attempt to apply glass on top of the powder without wiping off the excess layers, the glass will just fall off, because it will only have stuck to the outside layer. Mica Powder that is encased is protected from the flame and will not burn. The color of the glass that the Mica Powder is applied to affects the final look. You can do a quick color test by simply coating the end of a glass rod. Even if you do not encase the glass after coating it, you can wipe off the excessive layers of powder to see if the application was successful.
You can also make a glass rod with Mica Powder dispersed throughout it. Heat up a quantity of glass until molten. Mash it flat. In the center of the flattened glass, place a small amount of Mica Powder. Without spilling the Mica Powder, heat the opposite side of the glass in the flame until it becomes soft and pliable. Carefully fold the glass, trapping the Mica Powder and sealing it in and away from possible direct contact with the flame. Do this while forcing out as much air as possible. Using the glass rod that the original flattened glass came from, as a punty, and another glass rod, mix the glass in the flame until well blended. Pull out into a rod.
Regarding safety, we were advised to recommend that you use a dust mask when using micas as you would if using powders or frits.
Thanks, Pippa
Warm Glass sell Mica Powder/Pixie Dust, (amongst other glassy things) - and that is what joycelo has used to create the shimmer on her beads which you asked about.
Here's a link
http://www.warm-glass.co.uk/Shop/CategoryProducts.aspx?CategoryId=114
Modified to add - Pippa you beat me to the post!!! Thank you for all of that info!
Wow wow wow!!! ;D Thanks pippa, I've just had a read - SO HELPFUL, and it has explained quite a lot for me so thank you!!!!
I look forward to putting in an order with you very sooooooooooooooon :-D YAY!
And thank you for explain theflyingbedstead to me (sorry don't know your name) ;D ;D ;D
THANK YOU !!!!!!!!!!!!!! xxx