Hey
I wanted to have a go at making trollt ype beads withthe big mmetal cores how do i do this? cani buy the metal cores and and certain mandrals to just add glass or would i need to make the coes (i hope not... lol)
thanx
am hoping it might get me back into bead making again and i might actually practice enought o make osme decent beads!
Sam
you can get 5mm mandrels from Martin
Hi Sam,
Martin also sells some silver rivets which can be glued to a bead if you don't want to make the silver cores yourself! Here's a link to his website, http://www.tuffnellglass.com - look under Bead Making Equipment they are on the 3rd page.
so i can buy the 55m mandrals then stick the silver core int he middle?
Quote from: darm on March 02, 2009, 05:37:14 PM
55m mandrals
5mm - don't think he does 55m ones! :D but yes, you can stick the core in