Hi,could anyone tell me what thickness copper sheet i will need for jewelry making ,thanks Parin.

mizgeorge

Piece of string question - you can use anything from 0.1mm up to 3mm+ depending on what it is you want to make. Did you have any particular styles or techniques in mind?

the lady with the lamp

Hi,just bead caps for now but want to make alsorts of jewelry when i get more tools,thanks Parin.

mizgeorge

for caps, anywhere from 0.2mm up to about 0.7mm. If they're going to be etched, or otherwise surface treated, they need to be in the upper range.

the lady with the lamp

Thanks will order some thicker copper, cos im goimg to put a pattern on them,Parin.