Quote from: Black Heart Beads on August 19, 2010, 06:26:37 PM
>:( >:( >:( >:( Just got an expensive sheet of this in today's post :'( :'( :'( :'(

If you've not opened it maybe you could return it?  :-\
Hazel x

Chameleon

I dont know Trudi, I havent tried it on the surface, I have only had a little play this week for an idea im working on so Im a beginner on that too lol cant wait to see what you make  ;D

As far as the copper stuff goes, as soon as i have used it with any colour glass at all no matter how pale I loose all and any colour from the dichro so for me the only way to use it is with clear but not exactly versatile.

cwest

Complete waste of money, for me anyway. Followed the video instructions exactly, but the colour would not come off the copper. But I have lots of coloured bits in the bottom of the packet! I tried using these bits like frit, but it just didn't work.

Carolyn

sarah t

well done jeff.... best results i have seen so far ...as i have a load of it left i will try the method you used to see if the results any better ...i really hope so  :(