has anyone used one ?? .....i would love some feed back
got a tut for using one ??.......i would love to know how i am supposed to do it !
got one they want to lend /sell if i can get my hands on any of the above ??....i would love to try one ;)
I've got a donut press and what works for me is to start with two spacer beads and slowly build up dots north and south of the beads. I then use a knife to start moving the columns of dots towards one another. I keep putting the whole lot into the press so that I can see where I need to add extra glass. hope this helps.
Hi Sarah,
If you PM me your emailaddress I can send you some tut's for using the Doughnut.