Great stuff - I'm not an annealing guru, but whoever tackles this, as part of a quickie FAQ at the bottom or something: just *when* is it safe to snatch beads out of the kiln when it's cooling down - for us impatient ones? :o) (Sabine)

FAQ

I have had a go at adding the FAQ about how soon to remove beads. As far as I am concerned the information is correct. But please feel free to comment or edit if you disagree. --Dickie 23:13, 13 November 2008 (UTC)