Foodsafe Over glaze where is the best to get it in the uk.

Started by Jules1971, March 25, 2017, 02:21:37 PM

Previous topic - Next topic

0 Members and 2 Guests are viewing this topic.

Jules1971

Hi Guys where is the best place to buy in the Uk to by a foodsafe overglaze for bottle slumping.

Thanks all

Moira HFG

I must admit I am stumped here, I didn't know you needed any sort of overglaze on a slumped bottle.  ???

Jules1971

Hi moira it isnt so much that you need one i want to get a good glaze on some of my slumps especially if im going to use them for food.

Thanks Julian

flame n fuse

bullseye glass recommend a layer of clear over the coloured layer, but I don't know what you'd do when your base glass is of unknown coe

Moira HFG

Yes, quite so. You might get away with a bit of frit to decorate the surface, up to 5%, but any more and it's likely to crack as it cools.
Most bottles that people slump were made for wine or other drinks, so should be fine to use for food.